Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Selecting a Moisture Meter       A discussion of desirable attributes for a moisture meter used for kiln-drying quality control. June 30, 2007

Question
Anybody have a recommendation for a moisture meter that is not real sensitive about a consistent temperature (warmer than my shop typically is) and will not break the bank?

Forum Responses
(Sawing and Drying Forum)
From contributor J:
I just bought a Timber Check meter, which is simple to operate and can be had for $60. It is calibrated for 20C/68F, but it came with charts describing adjustments for other temps. Having to consult a chart is not ideal, but I think sensitivity to temperature is inevitable with electronic meters. Perhaps fancier units allow you to key in adjustment factors such as temp and species?



From contributor D:
Certainly Delmhorst, Wagner and Lignomat have stood the test of time. Over the years we have tried a number of meters and not found anything that stands up as well as these. Since meters are a very long term investment, it helps if the company making them stays around. A couple of years ago, someone from China was walking the IWF show in Atlanta and trying to sell various instruments. One was a moisture meter that would cost us about $15 and looked to be equal to anything out there at $150. He gave us 3 to try. Not one worked. Not even close.


From Professor Gene Wengert, forum technical advisor:
As some of you are aware, we ran tests on over 150 pieces of lumber using the Wagner, Lignomat and Delmhorst meters and then compared their results to the oven-dry values. The tests were done at room temperature with essentially no moisture gradients in the pieces. These three meters were quite accurate in almost all cases. (See results in the appendix in "Drying Hardwood Lumber".)

Because the density on an individual piece affects the Wagner, we did see some variation in that meter, as we did not fine tune the readings for density variation in the lumber. On the other hand, the Wagner was able to measure under 6.5% MC accurately, is very fast, allows scanning of the entire piece, and requires no temperature correction. The pin meters, which can measure gradients and have no concern about density variations, do not do well much under 7.0% MC, measure only at one spot, and require temperature correction (1% MC for every 20 F).

In truth, the best moisture meter is actually having both the pin and pin-less.

The minimum cost for a meter is around $200 if you want reliable readings and durable equipment with good resolution. Of course, if all you want to know is if the lumber is under 10% MC, then cheaper meters can be had. But I know that over-dried lumber is as bad as under-dried and that you really need to have accurate readings if you will use the readings to make some processing decisions.

We have also tested some other meters (six so far) made by other manufacturers and they often are 2 to 3% MC off. Perhaps the foreign manufacturer does not have the American species to use for calibration.

Although automatic temperature correction for the pin meters is not necessary, it is sure handy. Automatic species correction is also very desirable.

With a pin meter, it is fairly important to have insulated needles so you can measure moisture gradients and also get good readings even when there has been surface moisture regain. Most companies sell a separate probe for insulated needles.

Of course, with any meter, make sure that you can get replacement parts and service easily. I do know that two of the bigger companies (and maybe all three) will send you a replacement meter on loan if your meter breaks, so you are without a meter for 24 hours.

Finally, if you are selling lumber, it would be prudent to specify on the invoice or P.O. how you and your customer will be measuring the MC (meter brand, model). If your customers use a cheap meter, it is likely that they will get bad MC readings even though the wood is just fine.

Finally, it is critical that any meter be used. It would surprise you how often I see meters at companies that have 1/2" of dust on them.



From contributor O:
I have great luck with my Lignomat. Around $200, no problems, just change battery. Great investment.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Air Drying Lumber

  • KnowledgeBase: Primary Processing: Kiln Operation




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article