Question
The recent "Filling Glue Bottles" post got me looking into these systems. Has anyone had any experience with the GlueFast system? I am waiting to hear back on price and availability. The Pizzi systems look fantastic and I am sure over time pay for themselves. I was doing a little investigating as the initial investment is a tough one.

Forum Responses
(Architectural Woodworking Forum)
From contributor H:
I have a Schneeberger system and itís great!



From contributor O:
I think, depending on the work you do, a glue pot pays for itself very fast. I have the small Pizzi glue pot that holds about a gallon. While laminating plywood panels last year it was nice to never run out of glue in the middle of a panel. There are many attachments that can be used for specific jobs and they help to get the right amount of glue in the joint which saves time cleaning squeeze out after the fact and prevent weak joints when not enough glue is applied. It's one of those tools that once you have one you wonder how you ever got along without it.


From contributor H:
What about cleanup of the glue pot? Does it have to be done with every use or can it sit for weeks or months in a sealed condition? We have a couple hand held pot rollers we stopped using because cleanup was a pain.


From the original questioner:
I can easily see the advantages of the pot. What got me thinking is we were just doing a large batch of hand rail glue ups and itís always a chore. The Pizzi is head and shoulders above the glue-fast system I mentioned and when the P&A came back it was the same price so the Pizzi is the no brainer.

Itís just one of those hard decisions in the shop where the economics can be there but breaking off the $1K is a tough one. I will definitely be looking for a job to bury one of these systems, or part of it, in.



From contributor O:
The pot can sit for months with PVA glue. I keep mine filled with Titebond III. It is just like leaving the glue in the bottle as only the glue exposed to air dries. That said I have mine sitting unused for a few months and will check it out to see the condition. I do keep the glue gun end submerged in a container with water attached to the side of the glue pot. I fill this every couple of weeks when the water evaporates. Even if the water completely evaporated it would only take a few minutes with a wire to clean the end of the glue gun.


From contributor E:
I have one, and to answer your question, there is no clean up. The tip of the glue gun itself is submerged in a water container attached to the pot. Just give it a squirt to get rid of the diluted glue and get back to gluing.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Adhesives, Gluing and Laminating

  • KnowledgeBase: Adhesives, Gluing and Laminating: Gluing and Clamping Equipment


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2018 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article