Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




Showing Off Sycamore       Sawing and drying pros show photos of sycamore (quartersawn, spalted, and clean-shaven). February 14, 2006

Question
Does anyone have any nice pictures of sawn sycamore? I'm trying to decide if I should try to get a few logs that recently died from the drought here and pay to have them sawn. Is sycamore easy to air dry?

Forum Responses
(Sawing and Drying Forum)
From contributor A:
I love sycamore; it is great to work with, especially with hand tools. It is stunning when quarter sawn.




From contributor B:
Quarter sawn sycamore:




From contributor C:
Quarter sawn sycamore:




From contributor C:
Spalted sycamore:




From contributor C:
Quarter sawn and spalted sycamore:




From the original questioner:
How easy is it to dry? My sawyer has a vacuum kiln. Should I have him run it through the kiln, or just air dry it? I can easily get it to 12 percent or maybe lower where I live by air drying in my barn.


From contributor D:
Sycamore goes nuts when drying it - you need to weight it down or clamp it.


From contributor C:
Sycamore finishes out pretty well. When sawn green it does move quite a bit. When spalted, it just lays there and takes the sawing just fine. Quarter sawing aids in making it lay flatter and adds to the looks quite a lot.




From contributor E:
I saw Doug Stowe, a nationally known Eureka Springs Arkansas wood artisan last Saturday. I took a picture of a few of his little boxes that sell for mega bucks and this one happens to be QS sycamore. The picture does not do the box justice.




From contributor F:
Here is a sycamore domino box I made with Mesquite accents. The reddish swirls are heartwood. This was from an 8" limb I sawed on my Delta bandsaw before I got my mill.




From contributor F:
Here is a better one -




From contributor G:
Here's a little box I made from sycamore.




From contributor G:
Here is the inside.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Air Drying Lumber

  • KnowledgeBase: Primary Processing: General

  • KnowledgeBase: Primary Processing: Sawmilling




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article