Question
I am a one man shop building furniture and cabinets. I presently have a couple of conversion HVLP guns running off my compressor, which are okay for WB pre-cat lacquer, dyes, etc.

I am working on a job where the specified finish is Olde Century WB acrylic latex paint. I've sprayed latex paint before with my guns with a 2.2mm tip and it worked marginally, at best. I always seem to get it done, but it's touchy and takes some time. Is there something that would work better for spraying latex paint and not cost too much (maybe less than $500)? I could justify it on time savings and a better finish.

Forum Responses
(Finishing Forum))
Acrylic latex on furniture or cabinets? Won't they be happier with lacquer tinted to the same color as the latex spec? If you absolutely have to, you can rent latex spray setups for way less than $500.



Try thinning the paint some and spray with the biggest needle and tip you can. Have you thought about rolling the paint on? Or, ML Campbell makes a water based product called Polystar that is available in about 8 million colors, and I think they will even mix to match. It works great, lays flat, smooth as lacquer when done right and it doesn't look thick like paint.


If sticking with the latex, airless will be your best bet. You'll have to decide if you want to make a longer-term investment or purchase a setup for this job only. Most airless setups will work the same in putting down a finish. What you mainly pay for is volume output and longevity. The airless rigs that painting contractors use have large motors, larger pistons, and can be rebuilt after 500 - 1000 gallons.

For example, a Wagner Paintcrew will give you a good finish, but cannot be rebuilt and is garbage after 100 gallons. They run about $180 (plus $25 for the tip you'd need). Or for $100 more, Menards has some homeowner models that will last longer and give you better performance. But for $500, you can get a used pro-quality machine on EBay. It is important to get the right tip and filter for the gun. I would suggest a 210 and/or 311. (Not the 517 used for walls!) I have not used it, but there is a fine finish tip for lacquer, varnish, stains and all other fine finish coatings. Might work for latex as well. I would suggest you go to a local paint store like Sherwin Williams, ICI, or JC Licht for a rental unit to test it out. Should be about $50 to $75 for the day.



Latex paint with a topcoat of clear w.b. urethane or acrylic (for durability) makes a beautiful and easy finish. Just thin it down.


2.2 tip is what is giving you the marginal results. You are probably getting orange peel.
Thin the paint (30-40% until it gets to 18 seconds in a #4 ford cup, then use a 1.5 tip). Results should improve dramatically. Also, use Floetrol additive, 5-10%. You'll have to put on an extra coat of paint to make up for the thinner.


I think the Spraytech/Wagner ED655 would be a good pump for you. It's in your price range, with gun and hose, will work fine with acrylics, capable of 3000 psi and up to a .017 tip, but you'll probably only need to use .010-.013's.. I've worked with plenty of painting contractors that use these for doors and trim work. You'll get an excellent finish spraying acrylics with dual orifice fine finish tips. In my experience, the flat tips always produce a softer fan than the reversibles, which still seem to have the sharp edges you get with most airless tips. The Graco tips run about $30, but they will blow out pretty quick spraying acrylic. I usually buy a new one for every job, even if it's only a few gallons, but they are worth it.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2018 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article