Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Tips on Large Tambour Construction       Old-fashioned yellow glue and canvas have a proven track record. January 9, 2007

Question
I am building a 60" roll top desk. Never built tambours longer than 47". Does anyone have thoughts on the optimum size of the slats (thickness and height) for a red oak tambour 60" wide by 34" high? I plan to contact cement the strips to artist canvas, unless someone has a better backer to suggest.

Forum Responses
(Furniture Making Forum)
From contributor F:
First of all, I would use yellow glue instead. When I make them, they look like the cross-section of a Kit-Kat bar. 3/4" at the bottom and 1/2" thick.



From contributor M:
Rockler has a cable system for assembling tambour rolls. I personally have not used it, but for a 60" tambour, I think it might work better.


From the original questioner:
Thanks for your responses. I will check into the cable system, but since all is built but the tambour and groove into the stiles and top rail, I may not be able to retrofit the unit for a track system.

I’m thinking that I may have made the rails and stiles that receive the tambour groove a bit too narrow. I hadn’t thought about how much I would have to beef up the thickness of the slats to facilitate that extra foot of length. I’m thinking that my best direction at this point is to lay out the widest groove possible with the largest radius possible at the bends and then to test what width of slats will work without binding. Binding is a bad thing with a tambour!

Pertaining to the yellow glue: will it stick to the artist canvas? I usually stain and clear coat the slats first to prevent any possible glue/stain issues, but might try a test tambour with yellow glue. Poly glue would work, but dealing with the foam between the slats can be a real problem. Spraying on contact cement is rather quick and easy, but I always worry about the slats letting go.

Someone told me a while back that he used duck cloth, I think, for his backer material. Has anyone tried this? I use artist canvas because it doesn't stretch much and lasts a long time. However, it is easier to find duck cloth by the yard than artist canvas.



From contributor F:
Please don't use contact cement. I said my slats were at least 1/2" thick, but the ends are cut down to about 3/8" to ride in the groove. I think the duck cloth will work fine. If you stain and finish the slats first, you won't have to worry about the glue. Just wipe up promptly. You don't need that much glue anyway. After you stain/finish the slats, just run a cabinet scraper across the back before you glue.


From contributor T:
You want to remember that this tambour curtain is going to be real heavy. If it slides well on the way up, it will come down really fast. Hafele sells a spring loaded cable gizmo that helps pick up weight on the way up and slows the travel speed on the way down. We've done these with the canvas backs and with laced shark leader (Real thin metal cable like the stuff that comes with Accuride cable style flipper doors).

You might also look at some old kitchen queens. They have a groove that is about 1/4 inch deep. This groove feeds into a round holding pond that is 1/2 inch deep. You roll the curtain up like a sleeping bag to load it, then pull it down into the groove.



From contributor B:
I built eleven 50" wide roll tops about 25 years ago. I didn't know what kind of canvas to use, so I took an antique tambour to a boat place and he knew just what it was. I don't remember what the canvas was called, but I do remember that it had the word "duck" in it. I did a lot of experiments with different glues, and to my surprise, the glue that worked best was... Elmer's yellow. 25 years later, I still have access to 5 of those desks and there are no problems.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Furniture

  • KnowledgeBase: Furniture: Custom Furniture




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article