Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Tips on Vacuum-Press Veneering       Entry-level advice on vacuum bag veneering techniques, and leads to more info. July 21, 2006

Question
I am looking to buy my first veneer press and I’m looking at the 10 cfm vacupress. I would appreciate any advice on any must have accessories (cutters, glue,etc) and tips on intro to veneering.

Forum Responses
(Cabinetmaking Forum)
From contributor J:
I had bought both self contained units (unit with its own vacuum pump) and the type that works off your compressed air supply. I feel after having both that I prefer the self contained unit is best due to having the problem of leaving my compressor on overnight. Too many things could go wrong such as air lines leaking and the hose breaking. I manage a large shop and there is always something going wrong when the air compressor is left on overnight unattended.

As for the process advise, use plenty of protection on all corners of the material you are clamping. I have replaced a many expensive bags due to the sharp corners piercing through the vacuum bag. Make all your bending forms with ridged ribbing (1 pc ribs, not an arched upper pc rib attached to a flat bottom brace). They tend to break or compress on my projects. Make a frame press table for large flat panels (a hinged vacuum sheet lid that seals to a vacuum table). It’s a lot easer than sliding large panels into a bag and getting the proper protection on the corners.

I like the clamping jig that you can use with your vacuum pump. They are handy for routing, assembly and cutting when you need that extra hand. Using just the bag for free form bending is one of my favorite things to do with my vacuum press. There is a lot of good info on the web do a search for veneer bending, vacuum pressing veneer.



From contributor S:
Welcome to working with vacuum. There are two DVD's that I would recommend buying that will explain everything you need to know to do anything from veneering to bending or working with curves and moldings. The first is called "Working With Veneer" and this is a complete guide from start to finish and it also explains the pumps and bags.

The second is called "Working In A Vacuum” it deals with curves and shapes. Both can be bought from vacuum pressing systems or at vacupress.com. As far as bags and pumps, you will most likely need two bags. 50" x 50" and 50" x 10'. I bought the inexpensive kit from http://www.constantines.com/index.asp?PageAction=VIEWPROD&ProdID=702.

It works great as a starter kit and I have used it on many projects and the pump can work just as well on the lager bags. I was planning to upgrade to the better pump but honestly the pump from the kit works so well I have no need to replace it yet and I have had this kit for two years now.
Veneer cutters and glues can be bought at vacupress.com as well.



From contributor L:
We've gotten far more use out of our vacuum system than I ever thought we would. I started with two different types of bag, one urethane and one poly. Hands down the urethane is better than the poly. We bout the 5x10 frame and built a table for it after having the bags for a year. It’s much easier to use for pressing mild curves, flat panels etc. We have the 3/4hp pump and it works OK but with a lot of use it runs quite hot, generally not good for motors.

We installed a muffin fan inside the case to help keep the temperature down. We also installed a small vacuum tank to reduce the number of start stop cycles the pump has to make. The tank is made from 4" PVC pipe and fittings. Get the videotapes they are very good. Especially the demo of wrapping maple veneer around the radiused edges of a circular tabletop. The pillows also work amazingly well to help support the inside of forms.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Veneer

  • KnowledgeBase: Veneer: Techniques




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article