I used a new four stage Wagner 4900 hvlp sprayer and enduro water- base. After spraying, I could see what looked like water spots when I looked really close. Someone who used to do finishes told me it was orange peel, and I that I had to get the gun closer - about two inches from the surface, otherwise you get orange peel or pitting. I have tinted zinsner sealer under the topcoat.

What’s the best way to fix this? Should I strip it with lacquer thinner and start over, or can I spray a matte coat of enduro or two and keep going? I only want to redo the few really visible areas.The enduro seems a lot trickier to use than some of the other water-base, but it looks great and I would like to stick with it.

Forum Responses
(Finishing Forum)
From contributor M:
I would suggest that you sand and recoat it according to manufacturer's recommendations (recoat time). You can probably use some 320 s/c paper and level the finish as best as you can without sanding through.

You probably had the orange peel happen because the gun was not atomizing the material well enough. Try practicing on some other material, with the same prep. You may have to cut the fluid back and move slower, or have a wider fan pattern with the same fluid setting. You want a nice wet coat as you lay it down. If that doesn't work, you may have to thin the material.

Have a bright light at a low angle to the work piece to see how the product is laying down. I would also suggest taking a look at Wagner's recommendations related to distance from work piece. I am assuming it is around 8", not 2".

From contributor P:
Try thinning the finish with a little water (5% -10%). I routinely thin my water-base with 15% water because I like the way it helps it atomize and keep the coats thin. I've used it with 2 and 3 stage turbines with excellent results.

I've never tried getting as close as 2" from the surface, so I can't comment on that other than to say the fan must be about 1"-3" wide, and that's a lot of spray passes. I'm comfortable with 5"-6" from the surface using a turbine and 7"-8" with other spray systems.

I agree with sanding out the orange peel. If the coat isn't thick enough, don't try to level it out right away - sand it back and spray another coat. Then sand it again and level it out if the finish is thick enough.

From contributor A:
These responses have nailed it on the head. The turbine systems are very tricky to get dialed in, and the set-up will change with different materials, temperature, humidity, and so on. You have to play around to figure out the perfect set-up for you application.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article