Usefulness of Alder Wood

      but it has its own good and bad points. June 28, 2005

I am looking for some information about alder wood. I am trying to find out what the density is, and what other more common wood can it be compared to. I presume it is a smooth grain wood that may be comparable to soft maple? I would also like to find out how stable it is, and if it is useful in building furniture. I'm looking to use it as an interior grade part in furniture. Any information would be appreciated.

Forum Responses
(Sawing and Drying Forum)
From contributor F:
I don’t know the scientific specs on alder’s hardness. It is stable and used extensively in furniture and cabinet making. At one time it was used a lot for the understructure in upholstered furniture (and probably still is). These days a lot of makers use it as a primary show wood, and it can be stained to mimic other woods like cherry. It certainly would be acceptable as interior furniture members.

From contributor K:
Alder is a hot commodity. It used to be a poor boys maple, but with the advent of modern milling and kiln technology it has come into its own as a hardwood for cabinetry and furniture. It even supports a market for character wood using the knotty, stained and void containing boards that used to go to the chipper. It finishes beautifully with a light color and tight grain structure.

It tends to warp as it dries, so if you are air drying you'll really need to sticker, strap, and weight it well. Alder isn’t very good in the realm of rot resistance. If you use it for furniture, use it indoors only. Under moist warm conditions (underneath a bathroom cabinet) it will turn to pulp. The fully sealed/oiled cabinet door will be ok, but the interior face frame will rot.

From the original questioner:
Thank you for the information. This doesn’t sound like a wood I want to use for my application. Does anyone have any reccomendations for interior grade applications in wood seating that require a high degree of structural integrity (and wouldn’t set me back a lot)?

From contributor F:
To the original questioner: As far as the price goes, alder is usually one of least expensive hardwoods. Structural integrity will come from the method of building your seating. Oak is medium priced and would wear well as seating.

From Gene Wengert, forum technical advisor:
Alder is rather soft and dents easily. It is used as a substitute for cherry in applications where it will not be subject to denting. It is a rather expensive wood today, especially in wider sizes. Often, the grades are special grades owned by a company rather than the NHLA grades used for other hardwoods.

An excellent book “Utilization and Management of Alder” was published in 1978 by the Pacific NW Exp Station of the US Forest Service. Many libraries in OR and WA will have copies; your local library can probably get it through interlibrary loan from Oregon State university.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Wood Engineering

  • KnowledgeBase: Wood Engineering: Wood Properties

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article