How hard is persimmon to dry - is it like hickory? Also, how stable is it and would it make a good floor? Any help is appreciated.

Forum Responses
(Sawing and Drying Forum)
From contributor W:
I cut and dried some 9/4 for a gentle man and it was not very easy to dry. It was prone to cracking, but that was thick stock in 4/4. It may not be nearly as bad for you. It is very hard when dry and would wear well as a floor, but it’s not easy to get any amount of it in my area.

From contributor A:
It must be pretty hard and durable. When golf club heads on drivers and fairway woods used to be wood rather than the metal of today, they were often persimmon.

From contributor T:
Hickory might be a decent parallel. Put lots of weight on it because it likes to twist and warp.

From contributor R:
When I was scavenging through eight acres of pecan that had been bulldozed down to burn, a different tree on the ground caught my eye. The wood was very yellow. I cut about a 4 foot piece off the main trunk and later found someone to tell me what it was because I didn't know – and it was persimmon. "You'd better go back and get some more of that," he said. I certainly did. The tree is about 14 inches in diameter and I now have three logs totaling about 16 feet in all.

From contributor E:
Persimmon is very hard to season because of loggerhead worms, knot-release splitting that can go full length of the bole, discoloration, decay, cupping and warping when dried after milling, and of course, checking. The only way to prevent all of the above is to properly cure the wood in log form.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Sawmilling

  • KnowledgeBase: Wood Engineering

  • KnowledgeBase: Wood Engineering: Wood Properties

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article