      Mulberry is nice for turnings, knick-knacks, and furniture. April 18, 2009

I have available two big mulberry trees. Has anybody used it for furniture or turning? Any info would be appreciated.

Forum Responses
(Forestry Forum)
From contributor K:
I have done lots of turning from it, and think it is great for that. It is unbelievably yellow when you are working it, but it turns a light to medium brown within a few months. It is easy to work with, and finishes well. There is a small medular ray flake that is worth planning for.

From contributor W:
Here in Sacramento, if you look on the streets, before they pick it up, you can get the mulberry burl chunks, that people cut off the tops of their tree. Usually, the pieces are riddled with gaps and holes, but the pieces large enough, make great pens and other small turnings. The wood is yellow, to almost a deep gold and becomes incandescent, once you polish it up to 12,000 grit micro mesh. Also because of the many years of various cuts, you get some incredible grain patterns. Good luck, on the larger stuff, I have not been as happy with it.

From contributor L:
I've used it for some frame and panel work and for contrasting elements and inlays on furniture. It works easily and finishes well and turns a golden brown with time. I had two big trees cut into 4/4 and air dried it. One of the logs had wind shake but the other was very nice.

From contributor F:
Mulberry is one of my all-time favorites. It will split if you put a nail in it, but that's the worst thing I can say. The wood is gorgeous! Deep brown when aged just a little bit. If well sanded and given a clear coat, it looks almost like tiger's eye.

From contributor T:
Here is some mulberry I cooked up. I allowed it to sit around a few months and incubate.

Click here for higher quality, full size image

Click here for higher quality, full size image

From contributor A:
I made a small bench out of mulberry. It was a bright, beautiful yellow when I finished it, but it has darkened to an ugly brown color. It's too bad it doesn't stay bright yellow.

From contributor L:
I've got a rocking chair I made 20 years ago that has mulberry trim on a maple frame. The mulberry has turned a nice orangish brown and has good luster. Osage is a close relative and has the same look but is much harder. I've got a mallet I made from it 25 years ago - same nice orangish brown, and I still use it today.

The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor A:
Mulberry is used for expensive furniture in Japan. It is especially highly sought after for tea ceremony instruments and the "go" board game. Lots of traditional furniture is still made from it. Some furniture makers use mulberry veneer over their furniture to make them look traditional. It is possibly the next most sought after wood after (now protected) keyaki, Japanese elm.

Comment from contributor B:
I have just severely trimmed my mulberry tree. It is 15 years old and so big it was unmanageable. I once read that in mediaeval England, mulberry was often used for making the famous long bow. It dries to a very strong timber and I have made many rustic though interesting walking sticks. I currently have four pieces set aside to try and reproduce a long bow. It turns well, even when green, but for timber it must be cut on the quarter.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Sawmilling

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article