Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Vacuum Press Bags: Buy or Make?       When you need a custom size, it's not hard to make your own vacuum bag. July 18, 2008

Question
Can anyone recommend a supplier for vinyl vacuum bag material? I would like to make my own. Also, what works best for seaming the bag?

Forum Responses
(Veneer Forum)
From contributor K:
I buy mine from a local automotive upholstery supply. They will also sell a contact type adhesive made for the purpose, although when you use it, it swells the edge and causes a lot of puckering, and doesn't look very pretty. Check your Yellow Pages for a local listing, but mine is Rushing Upholstery in Little Rock, AR.



From the original questioner:
Thanks! I'll check it out. I still can't believe anyone puts vinyl on upholstery. Makes me have nightmares about sticking to my mother's couch when I was a kid.


From contributor D:
I would buy the bags from the Vacuum Pressing Systems. The have polyurethane bags that last almost forever. Mine is at least 8 - 9 years old and has been used hundreds of times and still has no leaks. Also they carry the fittings and everything you can possibly need to do good veneering work. Sometimes it is just better to spend a little and not have the headache. You have to figure it takes up time that you could be making items to make up the bag, etc. These guys have already worked out the bugs. It saves you money in the long run.


From contributor K:
You may be right, but one size doesn't always fit every job. I have got bags that I have been using since the mid 80's, long before I knew about sources for fabricated bags, and I have done projects where I needed a 24' long bag. I found it easier to build the bag around the glued plies with sheet vinyl and carpet tape than trying to feed something that big and slippery into a bag.


From the original questioner:
Talk about cheap. I've made bags out of 6 mil plastic sheet, spray adhesive and duct tape. As a matter of fact, I cut an old liner out of a swimming pool and I plan on trying to use it for the bottom of the next bag I make.

Down below is the vacuum pump system I made for $150.00 from industrial surplus parts ordered online. It blows the doors off any of the other systems I've seen.

Don't get taken in by companies marketing vacuum systems directly to woodworkers. Every other type of manufacturer uses vacuum systems in some part of their process. We are the only guys paying top dollar for the stuff. And I buy plumbing parts from Home Depot for a lot of the vacuum systems too.


Click here for higher quality, full size image



From contributor M:
Another source that I've used is from canvas shops that do boat repair. They usually have 19mil vinyl (for windows) on a roll 52 - 54" wide. Relatively inexpensive and heavy enough for most work.


From contributor W:
I just made an oversize bag. Go to a cloth store. Clothworld here carries 10 and 20 mil clear vinyl. Home centers have vinyl cement in the plumbing department for making vinyl liners for shower pans. That said, if it is not a special size or use, get a urethane bag. I agree with the earlier post, they last almost forever.


From contributor B:
Check out and their companion site. They have pre-made bags in several sizes and sell the raw materials to build (make) your own bags. They also sell all the parts to make your own vacuum generator, either by vacuum pump or venturi style. They seemed pretty reasonable for all the stuff I purchased from them.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Veneer

  • KnowledgeBase: Veneer: Techniques




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article