Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




Veneer Tape Tips and Tricks       Advice on selection and use of veneer tape. March 31, 2008

Question
I just read a post somewhere recommending using distilled water with veneer tape. Using tap water might cause ghosting when the tape is removed. I don't do a lot of veneering, but I did use tap water with the tape on a current project. Appreciate comments before I go any further. I am a one man pro shop, so lost time is costly.

Forum Responses
(Veneer Forum)
From contributor E:
The distilled water is a precaution. Some veneers, mainly maples and other lighter colors, may discolor from any mineral content in the water. Showing where the tape was usually only after finishing. So I use only distilled water, now. Got away with it for years. If you do much veneer seam taping, a tape dispenser is a much needed option. Work goes much faster with it.



From contributor W:
Where do you get your veneer tape dispenser from, and how much do they run? All I've been able to find are outrageously expensive.


From contributor E:
The dispenser I use came from Vacuum Pressing Systems. It's a desktop model and holds 2 rolls of tape. I got mine a few years back when I had a veneer job to lay up 2,000 ft of veneer. Paid for itself on that job.

Yes, they're expensive. I think mine was $135, but if you do more than a few feet of veneering a week, they pay for themselves pretty quickly. Another advantage is, the tape comes off the dispenser with the correct amount of wetness. Once you use it, you'll forget about the cost and wonder why it took you so long before you purchased one.



From contributor T:
I have been using cellophane tape - Scotch tape - with excellent results. 3M brand seems to be my favorite. Cheaper brands don't stick well. Run a veneer roller firmly over the seam to make it stick tightly. Put it in the press right away. Sometimes I add a few strips across the seam just for good measure. It will lift some wood when removed but it is a miniscule amount, virtually invisible when done. My press maxes out at 22Hg.


From contributor R:
With regard to the ghosting that you see when you remove the tape, it has nothing to do with the water. Obviously if you have brown water coming out of your tap, then you may have problems. What you have is the glue residue from the tape that remains after it has been removed with a wet rag. When taping veneer, and boy have I taped miles of it, your safest bet is to wet the tape just enough to activate the glue. After pressing, you can either sand it off or remove it with a wet rag and putty knife. Now don't saturate the panel, because all you'll wind up doing is impregnating more glue into your grain. The rag or sponge or whatever you choose to use should be damp, not saturated. Rub the tape until it becomes transparent and carefully scrape it off with a putty knife. Let your panel dry and then give it a good sand. I think you'll have pretty good success. Also allow your panel to sit at least 24 hours before introducing any moisture. This gives the glue ample time to cure and minimizes any chance of a de-lam between your substrate and veneer.


From contributor D:
I don't know if anyone has tried this, but I picked up an old butcher's tape machine off eBay that has worked well for me. It feeds the tape through water in lengths from 3 to 6 inches long. You just push down the lever and out comes the wetted tape. It works on all but the really thin perforated tapes. Saves a bunch of time and is around $30 for a good used one on eBay.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Veneer

  • KnowledgeBase: Veneer: Techniques




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article