Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




What Causes Burl Figure in Wood?       Nobody really knows why some trees form burls, but that doesn't stop us from speculating. December 28, 2006

Question
I love sawing burls and selling them, and over the years I have accumulated many different species and varieties of grain patterns - spalted, eyes, flames, and curls. Every individual burl is unique and has its own character. It seems that burls are caused by broken branches, insect damage, and many other sorts of distress to the tree. Does anybody know exactly how a burl forms and possibly how to force a tree to start forming one? It also seems that in my area (NJ), most maple trees in cemeteries are absolutely littered with burls - what could cause this? Something to do with underground nutrients for the tree? Also, why do some trees produce sphere-like burls and some almost pure burl, from the roots, to the trunk, to the branches?

Forum Responses
(Sawing and Drying Forum)
From contributor J:
I did a casual search of this once and found a lot who claimed they knew, but none were backed up by research. In addition to the insect and physical damage you mentioned, some think burls may be related to genetics or some type of fungus. Others have made observations that there are an abundance of burls in specific areas or groves, suggesting possible genetic susceptibility, but it seems to me that could just as easily be from localized damage from insect, bird, or fungus. (Maybe burls are caused by cosmic rays or fairy dust!)

The possible soil and chemical means you suggested is interesting, as is the cemetery observation; I suspect no one has studied the contribution of minerals from bones or other substances from buried mammals!

If you do find some real science concerning burl formation, please pass it on! I have black cherry, maple, oak, yellow poplar, and sassafras with burls and/or burl figure on my property and am also interested in propagating burls. I want to set up some controlled experiments including deliberate bark and under-bark damage, perhaps by injection. Another thing that occurred to me to try was to extract small plugs from an existing burl and implant them into an unaffected tree, a type of grafting.



From contributor A:
Nothing scientific, just from my experience of checking out soil problems in orchards. I have noticed burls on walnut trees, and the cause was possibly disc damage, or tractor hitting the base of the tree. Many times I have seen the base of the stumps that have had many years of disc damage. I have had my eye on a couple of walnuts that have a base of about 4 foot diameter, but that's only the damaged area. From the base (dirt level) up, say a foot, the trunk of the tree is only about 1.5 foot diameter. Every corner of this guy's orchard has trees that are in the same condition. This is where his disc scrapes the edges when he make the turns. His orchard is about 40 years old. Anyway, it's a good idea, forcing burl wood... Planting for the next generation's income source.


From contributor T:
There is some information on the subject at www.ag.auburn.edu/aaes/communications/bulletins/figureinwood/

This document is well worth reading for anyone interested in figured wood. On skimming, it appears to be an excellent reference defining the various types of figure encountered in wood and the underlying wood structure.

However, concerning burl formation, the author indicates what I've found elsewhere, stating "the ultimate cause of figure in living trees is largely unknown" and goes on to list various possible causes that have been suggested, some already noted in this thread. The author does mention the considerable interest in figure formation in the 1930's and '40's and includes references that would be interesting to track down. Also discussed are a number of things reported to affect the growth (not the initiation) of burled wood as well as information that appears to debunk some common misconceptions.

Of special interest is the chapter "Artificial Production of Figure", near the end, stating that while it would be desirable to artificially induce figuring in trees, "few successful attempts ... have been recorded." Some attempts and techniques are given, including one, shown in figure 52, a method to create "crinkle" by binding a tree with bamboo and cord.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Sawmilling




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article