What is the Hardest Wood on Earth?

      Trivia for wood lovers. There is some hard wood out there, people. April 11, 2008

I have a small piece of African ebony left from when I bought some about fifteen years ago. It's the solid black specie, not the striped black specie. I'm curious to know if it is the hardest, densest wood on the planet, or if some other species are just as hard and dense, or perhaps even harder and denser.

Forum Responses
From Professor Gene Wengert, Sawing and Drying Forum technical advisor:
Of the commercial timbers, lignum vitae is the heaviest, which is over 15% heavier than ebony.

Here is a quote from a US Forest Products Lab publication dated 1969...

"The most important and exacting use of lignum vitae is for bearings or bushing blocks lining the stern tubes of propeller shafts of steamships and submarines. The blocks are machined to conform to the curvature of the propeller shaft on one end-grain surface, and on the other side to conform to the curvature of the propeller tube. Numerous attempts have been made to substitute other hard, heavy woods for use as underwater bearings but none contain the high guaiac resin content which makes lignum vitae self lubricating and unique for this very exacting utilization."

From contributor A:
I read somewhere that some Bulnesia arborea from northern Venezuela and Colombia can be harder and heavier than Lignum. There are at least two sorts of Lignum, called ''male'' and ''female'' Lignum, female being lighter than male, I think. G. sanctum and G. oficinale.

From contributor V:
Takeshi Okuma, librarian at Camp Courtney, Okinawa, claims that the hardest wood in the world is Tiga, found in Sibuyan Island, Philippines. This island is reputed to have more indigenous flora and fauna than what Darwin found in the Galapagos.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Buying

  • KnowledgeBase: Wood Engineering

  • KnowledgeBase: Wood Engineering: Wood Properties

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article