Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




Working On-Site with Hardwood Millwork       Hardwood details add beauty and value to any installation. November 27, 2001

Hardwood Details Add Beauty and Value to Any Installation

Reprinted with permission from The Hardwood Council website.

Architectural details often are the perfect finishing touches to a truly outstanding home. Chair rails, crown mouldings and other decorative enhancements in oak, poplar, cherry, maple, ash, walnut and other beautiful North American hardwoods go a long way toward making a home into a showcase.

While these projects may require a little extra effort, they're well worth the time and investment. Here's how to work more confidently -- and economically -- with the quality hardwood products your clients demand.


Correcting Installation Blemishes

Even the most skilled carpenter can occasionally make a cutting, finishing or installation mistake during woodworking. Here are a few tips for correcting nicks, dents and other woodworking blemishes.

Applying Wood Filler
Sometimes, you may damage a piece of moulding with a hammer ding or dent, but it's difficult to get wood filler to stick to a very small blemish. To help give the filler an anchor, drill a couple of shallow holes in the dent with a 1/16" bit. These small holes will help the wood filler stay in place so that it covers up the blemish. Retouch all flaws with the matching stain.

Fixing Bad Cuts
If a slip of the saw damages an angled piece of moulding, compensate by making a clean cut on the inside of the defect. That's why specifying extra moulding in the planning stages is important. After attaining the proper angle, cut the moulding to fit by trimming the opposite end.

Using Wood Scraps
Never throw any wood away. Keep a scrap bin for large pieces and a milk jug for smaller bits and pieces. Scrap wood pieces often come in handy for decorative matching, contrasting parts, and/or screw plugs.

Putting Your Skills to Work on a Crown Moulding

Millwork projects demand precise craftsmanship, and a crown moulding installation is an excellent case in point. This project represents a variety of challenges, and the required skills can be transferred to any millwork installation, whether it's a chair rail, baseboard, window treatment, door trim, corbel, stair tread bracket or decorative medallion.

Pre-Installation Teamwork
Moulding installations run most smoothly when each member of the building team anticipates and addresses all elements and potential problems from the beginning. All parties should have drawings and specifications at the earliest stage possible. Remember that decisions and adjustments will affect the final installation and budget.

Check the specifications to figure the perimeter of each room and determine how many linear feet of moulding you will need. When ordering millwork, always add about two extra inches of moulding for each corner to compensate for any woodworking errors made during finishing or installation.

Millwork installation is normally one of the last steps in construction. Millwork orders should be placed at least six to eight weeks in advance. Be aware that the building team will have to agree upon, then choose, inspect and approve material samples before placing an order.

On-Site Layout
As building progresses, it is important to:

Visualize Installation and Restrictions -- When framing begins, document the precise locations of plumbing rough-ins, electrical and communications outlets, air grills and other obstructions that will affect the installation. Make any low-cost modifications before the walls go up.

Note Stud Locations -- Identify stud locations, wall and door frames, and ceiling heights so that holes can be pre-drilled before moulding installation.

Saw Angles and Related Moulding Positions
When cutting mouldings on a compound sliding miter saw, set the angles as directed in Table A and position the mouldings on the top surface of the saw base as indicated in Table B.

Table A

Moulding position in illustrationMiter AngleBevel Angle

?52/38? type?45? type52/38? type45? type

For inside corner
1
?Right 31.6??Right 35.3?33.9?30?

2

?Left 31.6??Left 35.3?

For outside corner3

?Right 31.6??Right 35.3?

4

Inside and Outside Moulding Joints
There are moulding joints made to fit inside (1&2) and outside (3&4) corners.

Table B

Moulding position in illustrationMoulding edge against guide fenceFinished piece

For inside corner 1Ceiling contact edge should be against guide fence.Finished piece will be on the left side of blade.

2Wall contact edge should be against guide fence.


Finished piece will be on the right side of blade.
For outside corner3

4Ceiling contact edge should be against guide fence.

Figure Corners and Measure Wall Angles -- Determine the number of inside and outside corners to identify the cuts you'll need to make (see illustration above). Also, walls are not always squared and true. Each corner will require you to measure the wall angles and figure the proper cutting angle. To do this, place a piece of moulding against the wall at each corner. Work with a small piece of moulding to easily see the angle and measure using a protractor. All angles will have a corresponding setting on your miter saw and the most common angles are detailed above (Tables A and B).

Cutting Angles
As shown in Tables A and B, there are two primary miter and bevel angle styles if the wall is a true 90-degree angle. Your installation angle is dependent on the size and shape of the moulding.

It is easiest to cut all mouldings on a sliding compound miter saw, placing the crown moulding with the broad back surface down on the turn base and setting the saw to the proper angle. If you use a standard miter saw, turn the moulding upside down and set it at an angle between the fence and the table.

Finishing and Installation
Mouldings and all other millwork can be ordered pre-finished or you may choose to site-finish before installation. Finishing details are offered in Pre-Finished or Site-Finished? Examining the Options.

Once properly cut and finished, the millwork is ready for installation. Pre-drill nail holes in all mouldings to avoid injuring the finish. Before nailing, apply construction adhesive to the mouldings where they will meet the wall and use wood glue in the mitered corners. Immediately wipe clean any glue that has seeped onto the finished moulding, wall or ceiling. Hold the moulding in place to give adhesives time to set. Then complete the installation by nailing the mouldings securely to the studs with a nail gun.

QuickTips

Pre-Installation Care
Proper preparation of the moulding and the worksite will prevent warpage and expansion/contraction damage:

--Store the millwork inside the house and off the floor to keep it dry.

--Run the heating/ventilation/air conditioning to bring the house to the normal relative humidity (normal conditions for your region) before and during moulding finishing and installation. Allow mouldings to acclimate for 3 to 5 days.

For more information, see Installing Hardwood Floors Over Concrete Slabs.

Saw Operation Caution
When making a cut, make sure the blade has stopped rotating before lifting it from the sawn millwork. Do not raise the blade while it is still rotating or the moulding will catch in the blade and be damaged.

In addition, when pressing down the handle, apply pressure parallel with the blade. A force perpendicular to the turn base or a change in the pressure direction during a cut will impair the precision of that cut.

Cutting Wide Miters
For installation of larger architectural mouldings (4 1/2" and wider), the compound sliding miter saw is particularly effective. This tool permits long, precise miters and allows you to work with the wood laid down instead of at an awkward angle.

Eliminating Miter Cuts
Beautiful miters accent the details of hardwood moulding, but crown blocks and other alternatives can eliminate the need to miter while still adding character to the trim. Crown blocks come as perfectly finished corners and make it easy to work on ceilings that have uneven lines.

Use rosettes and plinth blocks around door and window frames, and base blocks to finish the inside and outside corners of baseboards.

Installing Dentil Mouldings
If a moulding has dentil and embossing, match the dentil first and let the embossing match as well as possible.

Technical assistance and/or photos provided by: Ornamental Mouldings, Archdale, N.C.; White River Woodworks, Fayetteville, Ark.

? 1999 The Hardwood Council

Reprinted with permission from The Hardwood Council website.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Architectural Millwork

  • KnowledgeBase: Architectural Millwork: Millwork Installer

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article