Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




You say pecan, I say hickory       Pecan lumber is usually sold as hickory. June 20, 2000

Question
Since Hurricane Floyd, I have an abundance of pecan. I have cut it to 4/4 and am air-drying it. What are some possible uses, quality and market value? You never see it on the market.

Forum Responses
Pecan lumber is almost always sold as hickory -- this is legal and is traditional practice. There are four pecans and four true hickories that are sold as hickory lumber.

Hickory is used for tables, furniture, and a variety of other uses.
Gene Wengert



From the original questioner:
I couldn't find any info or anyone who knew what to do with it. I knew it was in the hickory family, but didn't know if the strength and characteristics where the same. It usually gets chopped up for the burn pile. I will have about 3000 board feet.

Sounds like it might be good for cabinet facings, doors, or floors.



Gentlemen, pecan is a hickory and is common all over the southern U.S. Pecan can either be sold as pecan or hickory, each has its own values/detriments. Here in southern Oklahoma we are blessed with massive amounts of pecan and hickory (and black walnut).


The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor A:
I retrieved a few pecan trees from a friend of mine who has a place on the South Llano River near Junction, Texas and took the logs to a sawmill near Cloudcroft, New Mexico. After they sawed them into 4/4 and 5/4 lumber, I stacked the lumber on strips for drying. It dries very slow. It also was bad to warp. After it dried, I made a trestle table (approximately 4' X 8') for the guy who owned the property where I got the logs. Also I have made several chests and other furniture. The lumber is very beautiful.



Comment from contributor B:
We used hickory in a custom built home that we used distressing on (hitting it with chains, ice picks). It was pretty difficult to work with but well worth the effort. When we started milling it my first thought was burning it was a good idea. But we got through it and when we were done, the cabinetry looked great. Plus, all the leftovers everybody took home and burnt in their fireplaces and smokers.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Lumber & Plywood: Wood Identification

  • KnowledgeBase: Primary Processing: Air Drying Lumber

  • KnowledgeBase: Primary Processing: Kiln Operation

  • KnowledgeBase: Primary Processing: Lumber Grading

  • KnowledgeBase: Primary Processing: Sawmilling

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article