Techniques for drying wooden bowls
Advice on how to dry large, turned vessels. 1998.

Honeycombing and Fresh Checking in a Newly Turned Newel Post
A woodworker's report of a honeycombing and checking problem leads to a good discussion of wood drying defects and how they manifest themselves. March 3, 2009

Lathe and Shaper Setups for Fluting and Reeding Columns
Jigs and rigs for fluting and reeding columns or posts using a lathe, shaper, or router. April 24, 2006

New turn on rosettes
Could cutting rosettes on a lathe reduce tearout problems? July 22, 2003

Machining Curved Crown Moulding
Pros describe how they manufacture small runs of crown moulding to curve around outside corners. November 8, 2008

Fabricating Large Wooden Columns
Brainstorming session about how to make 9-foot-high non-loadbearing decorative columns. February 5, 2007

Face Glue-Up Techniques for Making Turning Blanks
Woodworkers discuss the face preparation and gluing issues involved in making large blanks for turning. January 9, 2008

Glued-Up MDF on the Lathe
A woodworker experiments with laying up MDF blanks and turning them on a lathe. He reports mixed results, but says the idea has potential. May 6, 2006


Drying Large Rounds - Preventing Splitting
Is it possible to dry these without problems? October 20, 2003

Crown Molding for Radiused-Corner Cabinet Tops
An explanation of how to mill curved crown molding for application to radiused corners. June 23, 2006

Centered Drilling in Pole End Grain
Thoughts on how to drill centered, matching holes in the end of poles so the poles can be connected end to end. March 26, 2009

Dowel making
Machines and techniques used in dowel making. June 13, 2001

Eliminating Wood Problems -- An Industry Review: 10 Ways of Eliminating Wood Problems
Gene Wengert explains why eliminating wood problems begins and ends with monitoring and controlling the moisture content (MC) in wood -March 18, 2000

Today's Sponsors
  • Better Vacuum Cups, Inc.
    Vacuum Cups for All CNC Routers As Well As Many After Market Parts for Your CNC
  • Carter Products
    Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
  • Colonial Saw
    North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
  • Cabinetshop Maestro
    Web-Based Project Management Software for Custom Cabinet Shops - Manage Jobs from Prospect to Punchlist Through Scheduling, Task Management, Time Tracking and Communication
  • Biesse America
    Woodworking Machinery - Machining Centers, Edge Banders, Feeders/Stackers, Panel Sizing Centers
  • Safety Speed Manufacturing
    Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
  • NEMI
    Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
  • CP Adhesives
    Supplying Quality Adhesives to the Woodworking Industry
  • iBiDMachinery
    The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
  • Impact Search and Placement
    Professional Employment Recruiting Specialists
  • SAMES North America Corporation
    Precision Spraying Solutions From Pumps To Complete Application Systems-Design and Manufacture of Process Equipment Including Airspray, Airmix, Airless, Rexson Dispense, Electrostatic and Powder Coat
  • Template Services
    Professional Moulding Design and Template Making Service
  • Vexor Custom Woodworking Tools, Inc.
    Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More

Become a Sponsor today!