Sailboat masts
A discussion of species and techniques for seasoning wood used for sailboat masts. March 2, 2000

Structural Concerns for Boat Cabinetry
A proposal for a free-standing entertainment center on a boat sets off a discussion about appropriate technology in nautical cabinetry. July 30, 2007

Holly and Teak for Boat Decking
This thread answers the question of why Holly and Teak are paired in boat decking (below decks only), and continues with a folkloric and historic discussion of Teak for boatbuilding — including on nuclear submarines.October 19, 2013

Plywood and Lumber for Boat-Building
Thoughts on suitable wooden boat construction materials, and where to get them. May 23, 2007


Today's Sponsors
  • Better Vacuum Cups, Inc.
    Vacuum Cups for All CNC Routers As Well As Many After Market Parts for Your CNC
  • Carter Products
    Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
  • Colonial Saw
    North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
  • Cabinetshop Maestro
    Web-Based Project Management Software for Custom Cabinet Shops - Manage Jobs from Prospect to Punchlist Through Scheduling, Task Management, Time Tracking and Communication
  • Biesse America
    Woodworking Machinery - Machining Centers, Edge Banders, Feeders/Stackers, Panel Sizing Centers
  • Safety Speed Manufacturing
    Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
  • NEMI
    Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
  • CP Adhesives
    Supplying Quality Adhesives to the Woodworking Industry
  • iBiDMachinery
    The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
  • Impact Search and Placement
    Professional Employment Recruiting Specialists
  • SAMES North America Corporation
    Precision Spraying Solutions From Pumps To Complete Application Systems-Design and Manufacture of Process Equipment Including Airspray, Airmix, Airless, Rexson Dispense, Electrostatic and Powder Coat
  • Template Services
    Professional Moulding Design and Template Making Service
  • Vexor Custom Woodworking Tools, Inc.
    Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More

Become a Sponsor today!