Subject: Re: Millwork with Ipe

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Millwork with Ipe

4/23/14       
Geoff

I have been asked to price out a job of custom milling about 600 bft. with two different woods. One price is with ribbon sipo/utile and the other with ipe. I have never done any millwork with ipe and was wondering what to expect.
I guess it is worth mentioning that our shop mills a fair amount sipo and know what to expect. Also, we have a SCMI joiner and planer and two shapers.

4/4 sipo $4.45/bft rough
4/4 ipe $7.80/bft rough

4/24/14       #2: Millwork with Ipe ...
gary

Ipe is hard. REALLY HARD. Helical head would be preferred due to tear out.

4/24/14       #3: Millwork with Ipe ...
Chuck Rankin

Hi Geoff:

All I can say is carbide, carbide, carbide when milling Ipe. It is tough and heavy as well. They don't call it Ironwood for nothing. We have spec'd out a lot of tooling for Ipe over the years and carbide has always ended up being the tool of choice.

Best regards,

Chuck Rankin
Wood Tech Enterprises, Inc.
Phone (828) 628-4414

4/24/14       #4: Millwork with Ipe ...
Geoff

I failed to mention in my message last night that we have tersa cutter heads in both the joiner and planer.
I am guessing that the ipe dulls the knives quickly.
Do you get tear out planing, joining or both?

4/24/14       #5: Millwork with Ipe ...
Chuck Rankin

Hi Geoff:

We can supply you Genuine Swiss made solid carbide insert knives for the Tersa heads you have and most likely have them in stock. That would be the best option for the Ipe material.

Best regards,

Chuck Rankin
Wood Tech Enterprises, Inc.
P.O. Box 2226
Fairview, NC 28730, USA
Phone: 828-628-4414
Fax: 828-628-4490


View larger image

Tersa Knives

4/24/14       #6: Millwork with Ipe ...
gary

I have Tersa as well which is perfect for dropping in the carbide knives when you need them and storing when you don't. I have had mine for 5 years on one edge so far.

4/24/14       #7: Millwork with Ipe ...
Adam

Tearout is not usually a problem with ipe. Its so hard it machines like plastic.

Make sure everyone in the area is wearing a dust mask. The dust is toxic and can cause breathing problems.

4/26/14       #8: Millwork with Ipe ...
Steeliemark

Devil wood.
Hard, can splinter outrageously or fuzz at the other end of the same piece.
Oh my tired back heavy (well, ok, I'm an old man)
But it can look great oiled.
Carbide is the only way to go. I found that I would run high RPM's and a slower feed to mill it. Risk burns but I got a good finish with little sanding which is best because of the before mentioned nasty dust.
Devil wood

4/26/14       #9: Millwork with Ipe ...
JeffD

Adam has had better luck then me, I find Ipe to be nothing like plastic. It's incredibly dense, hard, and brittle. The brittle can be a problem as you can sometimes get large chunks ripped out when profiling. Even for simple stuff like rabbeting you need your cutters very sharp as it can tear out on you. This aspect also makes the splinters especially nasty. They tend to come off in long hard slivers and are more painful than typical domestic hardwoods.

The warning on the dust is right on too! When you mill the stuff you'll get this mustard yellow dust that is really pretty nasty. Oh and did anyone mention it's heavy….like really really heavy! I don't know how you add for that in the price….but I would! Moving 600 bd. ft. around is a lot more effort than moving 600 bd ft of say oak or even maple.

Might also be worth mentioning to the client some of the problems of Ipe, like if it needs any sanding on site it could be problematic. Or that it cannot be nailed or glued like normal trim but requires special considerations….ie, more expensive to install! Basically there's good reasons why you've never done any millwork with Ipe. It's simply best suited to exterior use….at least IMO.

good luck,
JeffD

4/26/14       #10: Millwork with Ipe ...
Adam

I guess we did have good luck with the ipe. I had expected trouble as you have remarked. We free handed 8 foot curves on the shaper for a massive pergola. No problems whatsoever. The posts were 12" x 12" x 10'. Thank god we had a forklift. I had to Mortise those bastards with a plunge router.

I hate ipe. Ipe decks feel like a concrete sidewalk under your feet. The handrails often endup with this awful splinters that cannot be sanded off.

4/27/14       #11: Millwork with Ipe ...
Geoff

Thank you for the responses to my question, it was the kind of information I was looking for.
I have worked with S4S ipe but haven't done any millwork with it. From my limited experience I was expecting it to be difficult to mill.
Hopefully they will choose a different wood. At this point I am suggesting pattern mahogany.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory