Subject: Re: Sauna wall panels

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Sauna wall panels

10/4/15       
Damir Dehlic  Member

A designer asked me to make some wall panels for a sauna similar to those in the picture.

Did anybody make some similar panels?
We are thinking of using a marine grade plywood for the substrate and gluing veneer with UF glue on both sides using a hot press.
Is their a better substrate for this application?

The sauna temperatures are from 50 degrees Celsius (122 Fahrenheit) to 80 (176 Fahrenheit) degrees and the air humidity is from 20% to 50% depending on the sauna type.

Thanks


View higher quality, full size image (1024 X 894)

10/4/15       #2: Sauna wall panels ...
Adam

Do not use epoxy resins. Typical stuff like West System start to lose mechanical properties around 120F and melt around 200F.

10/5/15       #3: Sauna wall panels ...
Damir Dehlic  Member

Thanks Adam.

I don't plan to use epoxy, it is expensive and takes a long time to cure.

I looked at some sauna panels and they were cracked because of the high temperature and low humidity.

This is why I plan to use thin veneer and a hard glue. I'm curious if there is a better substrate to use.

10/11/15       #4: Sauna wall panels ...
karl  Member

Website: http://www.benchwerks.com

Here are some Boat guys discussing MDO v Marine plywood.

I of course realize that you have the additional problems of extreme temp fluctuations, and they aren't talking about veneering, but I was interested in some of the opinions/experiences with regards to the paper, and thought it might have some application for you.

MDO v Marine Plywood

10/20/15       #5: Sauna wall panels ...
Gene Wengert - Wood Doc

Most common epoxy adhesives, once cured, can withstand 250 F to 300 F before they begin to lose strength. There are even epoxies made for high temperature use that go even higher. Note that this is "in use" but the temperatures for curing and post curing must be much cooler. The spec sheet for epoxy should give you the service temperature.

Wood is not affected by temperature changes, so the temperature variation you will have is not a problem with the correct adhesive. (If the temperature variation causes humidity changes, then there can be an issue...see next paragraph.)

Here is the problem, however. You will have a widely varying moisture condition, meaning that the wood will tend to move quite a bit. It is virtually impossible to stop this movement. So, we need to consider a wood species that is not prone to much movement. One species often used is aspen (also called aspen poplar, quaking aspen and a few other names). This wood is also splinterless, which can be an advantage in a sauna.

Marine grade means that the adhesive used is stable when wet (The adhesive is that same as used in CD-X plywood.) and also that the lowest grade veneer within the panel is fairly high quality (B grade or higher). The plywood will still move slightly with moisture changes. Some of the movement will be warping, so fastening the plywood to the frame is critical. You also want to leave room for expansion and contraction.

11/24/20       #6: Sauna wall panels ...
Lynne Member

Website: https://www.supawood.com.au/products/supaline/

I found some options for walls and ceiling panels. It is available in a variety of different finishes.They are also good for decorative panels for pillars or beams or office partitions.

11/24/20       #7: Sauna wall panels ...
GeneWengert-WoodDoc

The product you cited is not recommended for high humidity. Therefore, use in a sauna is inappropriate.

Further, I could find no information on heat limits. Also, the name is a registered trademark, so should have the R with a circle, or other designation. The product is wood and resin sold as a panel. It is made in South Africa. Is it available in the U.S.? What makes this different from other wood resin products...particleboard, fiberboard flake board, MDF, etc.?

1/10/22       #9: NotifyOnlyPost ...
Keystone Linings

Website: https://keystonelinings.com.au

I found good options for Acoustic Wall Panels and Ceiling Panels. It is also available in various dimensions with different finishes. They are also good for Acoustic Wall Panels and Ceiling Panels or office partitions.

Architectural Wall Panels Ceiling Panels

1/13/22       #10: Sauna wall panels ...
Xenia

Website: http://jgrabner.at

There are sauna panels - veneered plywood, suitable for sauna.
Water and heat resistant glue --> delamination warranty; fomaldehyde free (tested by T=90 °&#1057;). Big variety of wood species, textures and colours.
Check "saunaboard" on www.jgrabner.at.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!