Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Chargers in a bar top?a

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Chargers in a bar top?

12/16/22       
David R Sochar Member

Website: http://www.acornwoodworks.com

I am trying to get my local brewery to replace the old walnut stained, rotary Oak bartop and Chicago bar rail with an upgraded top in Maple, with the Keith Richard’s bar rail. And built in phone chargers, The phone chargers are a bit out of my league. I would prefer a continuous strip of the top that would be available whenever a phone was placed in this continuous “hot zone.” But It think they would have to be right next to each other, a5 about 10 chargers per 5 l/f of bartop. 2 per foot. Could I still get a charge at one every foot? For aesthetic reasons, there would be nothing in the bartop ditself that would indicate where the chargers are.

My other quandary is wiring. The chargers I have seen are all USB plug ins. I would like to have simple chained up female USB’s in one line, and plug in the charger and be done. But I don't see anything like this in my searches.

12/17/22       #2: Chargers in a bar top?a ...
Tom Gardiner

You could pop one of these every 48"

https://www.richelieu.com/ca/en/category/office-accessories/wire-manag
ement-and-grills/plastic-grommets/round-grommet-with-two-usb-charge-ports/1178343
/sku-7188102090

12/17/22       #3: Chargers in a bar top?a ...
Chris  Member

Website: rangate.com

HI David, if you are open to wireless charger, perhaps a removeable veneer or thin cover with a charging icon for each unit will suffice both the charging and service access need, without degrading the charging time too much. You will want to get them out first of course to see the material/slot shape/cover/charging performance. The placement positions need to be considered also - I wouldn't want the drinks to spill on my device as the bartender hands over my drink. Ha! It sounds like a fun project!

https://www.nytimes.com/wirecutter/reviews/best-qi-wireless-charger-fo
r-iphone-and-android-phones/

Qi Chargers

12/27/22       #4: Chargers in a bar top?a ...
David Sochar

Website: http://www.acornwoodworks.com

I think they need to be close enough to saturate the area so that a phone set down about anywhere will get charged. And all access from below to prevent spills from getting to it.

Also, the idea that it all be 100% invisible is important. I envision a 24’ long usb wiring harness that would feed 12 chargers, with easy connectors. Where could I find this, or have it made?

I would build it as 3/16” solids on top of 3/4 MDF, with 3/16 on the bottom. Hard maple strips 1-3/4” wide, with one full width 90 degree turn. Bar rail would be a 3” diameter solid rail set just above the top.

12/27/22       #5: Chargers in a bar top?a ...
Zach Member

Maybe something like this?

https://www.gordonelectricsupply.com/p/Wiremold-Wh20Usb512-Usb-Plugmold-5
Ft-Wh-5-Usb-Modules/5953489?gclid=CjwKCAiAy_CcBhBeEiwAcoMRHHKBZ9-vusRw4OeNDr_aM39
EN1PisRTsm8gw43BcUgHgAlJG2VEBuRoCqucQAvD_BwE

Zach

12/29/22       #6: Chargers in a bar top?a ...
David R Sochar Member

Yup, that would do it. Nice and neat. Expensive, but it would work.

12/30/22       #7: Chargers in a bar top?a ...
Joe

Perhaps this might be helpful?
https://www.onepointech.com/stealth-wireless-charger
What does a Keith Richards bar rail look like?

https://www.onepointech.com/stealth-wireless-charger

1/1/23       #8: Chargers in a bar top?a ...
David R Sochar Member

I used a 3" round rail, set low to the top, Enough to hold onto, but not to cut into your forearms, etc. The bartender told me that when the Stones stayed there for two nights, Mr Richards spent most of his waking hours in the bar, and commented that the bar rail was uncommonly comfortable, yet substantial enough to hold onto, when needed. A complement from no higher authority.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!