A thick epoxy question, not work related just rhetorical

8/14/18       
MarkB Member

So this morning we got yet again another request from a designer regarding "epoxy river tables". I almost throw up in my mouth every time this happens, which is a lot. But Im really wondering about a few things.

Does anyone have any real long term data on the structural adhesive bond between 2.5" to 3" thick epoxy and wood? And even more so sap wood?

We have never done any of these for a multitude of reasons. The main one being that everyone sees them on the internet and pinterest and wants one until they find out the two live edge slabs to make a coffee table may be worth 150 bucks a piece (if they are cheap), and the epoxy is $100+ a gallon plus colorant and metal flake, and so on. And you've yet to calculate a wood or metal base, at which point they click-thru on the pinterest link and see the coffee table they were enamoured by is $2600.00 and the dining room or conference table is 12-15K.

Regardless of the price. These things have always gotten me wondering if anyone truly has any long term experience with the bond between 3" thick epoxy and a wood surface? You have the mechanical keyed connection between the epoxy and any negative profiles in the live edge of the material but I have seen epoxy on many occasions delaminate on thick applications creating a kind of cloudy pocket or bubble where it has detached from the substrate. I have always seen some of these river table deals that have pretty smooth/sanded live edge and wondered if over time the live edge wont pop completely free from the epoxy or just as bad show a bunch of separation between the epoxy and the wood through the clear pour?

Beyond all that you see a lot of massive tables that seem to rely structurally on the integrity of the entire top solely based on the adhesive and mechanical bond of the epoxy to the live edge? I have seen massive conference tables with post bases that if that epoxy connection fails, the entire table is going to peel apart at the center, chopping anyone off at the thighs who is sitting their drinking their caramel macchiato.

Im thankful that every inquiry has not gone forward but I know the day is going to come when one will.

A small table doesnt worry me but the large requests we get concern me. We can always turn the work away but just like the requests will continue to come, the chance is the request will come on a job where we will want to take the money and just trying to get ahead of the curve.

8/14/18       #2: A thick epoxy question, not work re ...
Adam

How thick is the epoxy coating? If you get good bonds from epoxy, it is worth approx 3000psi in shear.

We use it to bond crazy loaded hardware directly to fibreglass sailboat boat decks.

The key is for the substrate to be stable. 80 grit scratches are all you need for proper "keying".

8/14/18       #3: A thick epoxy question, not work re ...
rich c.

I've wondered the same things. Besides the wood moving, polyester resin shrinks when it cures. That would make the bond even worse. I also can't imagine the resin will be so pristine after a year of people cleaning with the wrong product, or a slightly abrasive cloth. A nice wood slab will still be a good design in 10 years, a river table may not be.

8/15/18       #4: A thick epoxy question, not work re ...
Joseph

Website: http://eultgenwoodworking.com

My biggest concern for this type of construction is if the wood is air dried or kiln dried. I don't care if it's air dried for 50 years...its going to move and break all the bond lines. I could see possibly doing it with KD.

8/15/18       #5: A thick epoxy question, not work re ...
MarkB Member

These are all the issues I have had as well. I know epoxy has tremendous bonding strength. We use it quite often. But I have just never been able to get my head around the subtleties of the differential movement between a 3" thick epoxy pour (even in multiple lifts) and a 3" thick slab.

Agree on the air dried vs. KD and also agree completely on the cleaning, wear and tear, issues. I have had the opportunity to see a few of the clear acrylic desk stations that you commonly see on the nightly news and since HDTV has come along its a bit more obvious to someone who looks, but TV can make a scratched up plexiglass table look far better than it does in person.

The fad issue aside its just been something Ive been concerned about. We have typically tried to lean people towards a gapped live edge with a custom tempered glass insert in the gap mainly for the maintenance and durability issue.

8/23/18       #7: A thick epoxy question, not work re ...
Martin Quinlan Member

I often wonder whether those making these style of tables have any traditional experience in the nuances of jointing of large timbers.
I know working with one of our native species Red Gum, if it wants to go you wont stop it.

Marty


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!