Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Paint grade doors

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Paint grade doors

5/20/15       
Stewart Member

I'm looking for a source for cabinet doors where the stile and rail (or mitered) joints aren't so prone to yield hairline cracks through the paint. Is this possible? What have you guys found? Also, if you are using an mdf raised or recessed panel, are you caulking ahead of time? I prefer maple frames with mdf panels.

5/20/15       #2: Paint grade doors ...
Chris

It's a bit cheesy and lo grade, but I have cut a frame door (for glass) out of a sheet of 3/4 mdf because it was polished high gloss and I was worried about the hairline cracking at joints. I think anything that has a glued joint will eventually if not immediately show through the paint

5/20/15       #3: Paint grade doors ...
cabinetmaker

Stewart

The cracks will develop regardless in mortise and tenon stile to rail and/or a mitered door, period, its just a fact.

I have done what Chris has done many times, but if the client is after a paint and wants mitered or stile and rail, it's gonna crack over time and it's better to explain it up front.

Good luck

5/20/15       #4: Paint grade doors ...
JM

The only way to stop the hairline cracks is to use a 1 piece MDF door. Lots of options and styles available. Check out these guys http://www.cncwoodcraft.com/

As for the caulking of the panel to the frame, we dont caulk at all and really dont see the need, and also fear the caulk joint cracking over time.

5/20/15       #5: Paint grade doors ...
John Langley

This is only my opinion, solid MDF doors do not look real. With a frame and panel doors they look real. Yes you're going to get some hairline cracks don't forget your fighting Mother Nature if you want doors that don't crack Buy them at IKEA they're all plastic

5/20/15       #6: Paint grade doors ...
Gary

One piece mdf doors made on the cnc. Only way to go for paint grade in my opinion.

5/20/15       #7: Paint grade doors ...
Mike Fuson

I'm with John on this. Solid mdf doors look fake. I have used them exclusively in the past but now we do five piece with an mdf panel, which is the only way to go in my opinion. I don't use any caulk at all. Use space balls. Glue the joints and we use 5/8 brads in the back of the door to pin it.

5/20/15       #8: Paint grade doors ...
Leo G

Before you prime take 2P-10 and put a line across the joint, spray the accelerator on the glue and let it setup. Then sand it down flush. It'll keep it pretty solid.

The secret is to use 2 types of 2P-10. First apply the thin version, this will penetrate the joint, then cover it with the thick. This will now flow nicely across the wetted joint. Then spray with the accelerator.

I had to redo a kitchen that had bought doors. They only put glue on the tenons and none on the shoulder. I think a lot of them do that to lessen the chance of glue squeeze out. But it leaves the joint open to movement. Especially if they pin the back of the door in lieu of clamps.

5/21/15       #9: Paint grade doors ...
Mike

I like to mix MDF and maple; I cut the frame with a rabbet and center panel cut out of MDF, then set the MDF center panel in it, then use maple moldings for the outside edge and stile and rail profile.

For a cheaper easier route you can leave the frame and raised panel one piece (I like to put a route in the back so that it's not just flat) and just do the applied molding for the stile and rail edge. Either way yields a door that is indistinguishable for a non-mdf door, except for the lack of joints showing through.

That's the only way I can guarantee a door the won't eventually show the frame joints because there aren't any.

5/21/15       #10: Paint grade doors ...
gary

In our case it depends on the customer. As I said before I personally think solid mdf is the way to go but it is ultimately up to the customer. None of them, including myself has ever thought they look fake. Granted there is no joint or gap where the panel enters the stile and rails but in my customers' minds that is a plus. If they don't want solid mdf that's fine with us. We'll build what they want. I would say about 75% pick the solid mdf door because they think it is cleaner looking and easier to wipe down.

5/21/15       #11: Paint grade doors ...
Stewart Member

Thanks everyone for your help! I'm glad I'm not the only one that has had this issue. I very much appreciate the different approaches outlined here and will be incorporating several of them in our paint grade work - very helpful.

5/21/15       #12: Paint grade doors ...
matt calnen

I live in an northern michigan with alot of seasonal homes (aka, not heated in the winter). I have been making stile and rail doors out of mdf for years and they look as good today as when I built them. I clamp them 30 minutes with yellow glue, and I space ball the panels in the frame. Even when painted with lacquer, they still don't crack. I use plum creek mdf, two coats of primer and two top coats and the doors look great. I try to make my doors so they don't need caulk.

5/21/15       #13: Paint grade doors ...
Mike Fuson

Gary, fake might be the wrong word for me to use. It's the rounded corners that I don't like.

5/22/15       #14: Paint grade doors ...
gary

Mike, on some doors I've seen I would have to agree with you. When we make one piece mdf doors on the cnc the final clean up pass in the corners of the stick profile is done with a 1/8" diam. bit. That's 1/16" radius. Unless you specifically look for that small radius it is not noticeable.

5/22/15       #15: Paint grade doors ...
Stewart Member

For those of you who do the recessed panel doors in one piece mdf, how to you clean up the panel well enough to look good under paint?

5/24/15       #16: Paint grade doors ...
Mike

It's not the radius of the 1/8" bit people don't like, it's the rounded stile and rail profile at the corner that is the problem. I'm surprised there aren't smaller diameter bits for stile and rail available; they seem to be larger diameter probably for a cleaner cut at speed and for the larger flat area at the bottom for one pass machining. Compare the inside corner left behind from a typical round over stile and rail bit for mdf doors and one left by a pointed round over bit and you'll see what I'm talking about.

I haven't tried to make one piece flat panel doors for obvious finishing concerns, and the additional machining and finishing makes for a more expensive door than the raised panel variety. If I had to I would route a frame with rabbeted cut-out and drop a 1/4 or 3/8 panel in.

5/24/15       #17: Paint grade doors ...
Mike Fuson

The reason I got away from the one piece doors was the sanding of the profiles. It was time consuming to do the sanding before finishing. The mdf panel on a five piece is simple.

5/25/15       #18: Paint grade doors ...
Dave L

I don't get it, which part of this profile don't you like?


View higher quality, full size image (1280 X 960)

5/25/15       #19: Paint grade doors ...
JohnB Member

I am doing mostly pretty high end cabinetry for kitchens and MDF is a no-no word to many of my customers. They don't want to listen to reasoning of better stability, etc. We use maple and space balls for natural and painted, glue applied to both rail and stile, panels back pinned at center point, and have had minimal crack transfers. All frames are clamped for a minimum 20 minutes. But then again, we are also getting a lot of requests for brushed finishes so they can "see the brushmarks" to which I tell them, "we will supply primed and sanded, you hire a painter for after install"!! Makes my life even easier.
Occasionally we buy from Waltzcraft and have never had crack issues then either.

5/26/15       #20: Paint grade doors ...
Gary

Not saying my way is right and yours is wrong but I don't understand a couple of things..

Why do you sand the profiles? One reason we like mdf doors is there is no sanding. The finish off the cnc is great.

Why would flat panels be a problem? Minimal sanding with a square pad sander on the panel. High build primer and ready for paint.

5/26/15       #21: Paint grade doors ...
gary

Just to clarify, we do make flat panel doors the cnc. The cutter that hogs out the panel is 1 1/4" diam. so it doesn't take long. It leaves slight ridges but as I mentioned, a little sanding and high build primer fix that.

5/27/15       #22: Paint grade doors ...
JeffD

Count me as another guy going against the grain and making doors that don't develop cracks. It's a pretty extensive and top secret method that I'll share just this once. I glue them using TB1, clamp them for half an hour, and wait until the next day to sand…..oh yeah and there's the magic spell as well, but can't share that part:>0

If you turn a door and see pin holes in the back….pretty much guaranteed to develop cracks.

Funny thing is I just started working for a new developer. Guy bought the building my old shop was in to turn into town houses. While at my shop was looking at some old doors I had lying around and asked me why they didn't have those cracks;)

good luck,
JeffD

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello