Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Smallest Possible Gap Face Frame Hinge?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Smallest Possible Gap Face Frame Hinge?

8/24/15       
Pat

I have a client who wants to replace her kitchen doors and drawer fronts. The existing cabinets are face frame with 5-panel doors and she'd like to replace them with contemporary slab doors with tight gaps between doors.

I typically use Blum Compact 33 hinges for face frame cabinets, but the minimum gap on the hinged edge is 3/16". Is there a face frame hinge that allows a smaller gap?

Thanks,
Pat

8/25/15       #2: Smallest Possible Gap Face Frame Hi ...
Dan

Depends on your overlay. All the gaps on that type of hinge are larger. If you can use a standard euro hinge with a face frame plate you can get a tighter gap but it depends on the overlay.

8/25/15       #3: Smallest Possible Gap Face Frame Hi ...
Pat

The overlay will be close to the full width of a 1 1/2" face frame, so 1 3/8 - 1 7/16".

8/25/15       #4: Smallest Possible Gap Face Frame Hi ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Pat,

This is a common question and there is no real great solution. Although some face frame hinges give slightly smaller gaps than others, the difference is really splitting hairs. Salice is slightly better than most with a gap requirement of 5.2mm (5/32"). Keep in mind too that the 3/16 in gap requirement is per door. If you have a scenario where 2 doors are back to back the gap will need to be doubled (almost 1/2") to allow opening the two doors at the same time.

Also, the gap required between the door and the face frame is also much greater for compact style face frame hinges. This will be particularly noticeable at the end of a run of cabinets. Many people find this objectionable.

As Dan mentioned, using a standard Euro hinge and a face frame adapter mounting plate can produce very small gaps (1/8" or less). The problem here arises with the overlay. Without considerable modification to the face frame the maximum overlay will be somewhere between 3/4" and 15/16" depending on the hinge you use. If planned correctly this can also be worked out by hinging the doors on common frames back to back as in the example below. Each door overlays 11/16" with a 1/8" gap between doors.

I would do one of 2 things. First, I would build a small mock-up using compact hinges and show your customer the results. I might also suggest the customer go to the local big box store kitchen department and look at the displays. Most of them today use 1-1/2" frames with 1-1/4" overlay compact hinges to get that "full overlay" Euro cabinet look.
If the gaps she sees between the doors there are acceptable then you should be able to proceed using any compact hinge and give her the same results. This may be all she is really expecting.

Another point to check is the corner cabinet if there is one. If it is pie corner application then a 165 degree hinge would be best. You will need to do the same overlay planning here as with the other doors. There are a couple of solutions for this.

I might also ask if she would be interested in self close doors or soft close doors.

Best of luck.


View higher quality, full size image (774 X 1142)

8/25/15       #5: Smallest Possible Gap Face Frame Hi ...
Pat

Thanks, Dennis.
This is pretty much what I expected, but I was hoping that someone had introduced a FF hinge with some fancy articulation that solved this.

8/25/15       #6: Smallest Possible Gap Face Frame Hi ...
Bruce H

Build her a new kitchen. Retrofitting a Model T to Ferrari standards isn't going to be practicable.

8/26/15       #7: Smallest Possible Gap Face Frame Hi ...
matermark

Blum 38/39 series compact faceframe hinges are available in 1-1/4" plus can adjust up to another 1/8" I believe. They may make 1-5/16" or 1-3/8", I'm not positive and don't have a Blum catalog handy...

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello