Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: What species of wood are you using for painted cabinets?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

What species of wood are you using for painted cabinets?

8/25/16       
Brett

Hi,
I'm just wondering what type of wood species you guys typically use for painted cabinets? We have used mostly poplar for as long as I can remember but we have had a couple of problems with the doors warping with the last couple jobs. Some doors that are perfect will end up warping a few months down the road. One of these jobs happens to be inset so you can imagine what a slightly warped door is going to look like. We sub out most of our doors and they have a "paint grade" species that we always use for painted cabinets. This seems to be a mix of mostly poplar with some soft maple mixed in. Would it be the poplar that is warping or maybe a bad batch of lumber? We're possibly thinking of going with all soft maple doors for painted cabinets but would appreciate any of your input.

8/25/16       #2: What species of wood are you using ...
Wyatt

We use soft maple. We have had the same problem with poplar in the past. I told our door company if any doors show up made out of poplar I will refuse them. That stuff just isn't stable.

8/25/16       #3: What species of wood are you using ...
Dennis

I also use soft maple for paint grade doors, aside from the potential for warping, poplar is just too difficult to get a smooth finish on. You can use a "paint grade" maple which has too much color variation for staining but works fine for solid colors.

8/25/16       #4: What species of wood are you using ...
Adam B Member

Brett,

have you ever tried/considered 1 piece MDF doors?

8/25/16       #5: What species of wood are you using ...
JeffD

Soft maple here as well, poplar it just not the best wood for better quality cabinet doors.

good luck
JeffD

8/25/16       #6: What species of wood are you using ...
Leo G

Paint grade is soft maple and I mostly use an MDF panel.

8/25/16       #7: What species of wood are you using ...
Edi Silva  Member

Website: silvawoodworking.com

Soft Maple and Mdf for panels, we primed our panels prior to assemble the doors also.

8/26/16       #8: What species of wood are you using ...
Brett

Adam,
We have considered 1 pc. mdf doors but we have yet to try them. I'm not sure mdf doors would be as durable though. I would be worried about the corners chipping in a heavily used kitchen but maybe I'm wrong. I think we may try soft maple and see if we have a better outcome than poplar.

8/26/16       #9: What species of wood are you using ...
Tony

Definitely soft maple. The grain in poplar will telegraph through the finish no matter how well it's prepped.

8/26/16       #10: What species of wood are you using ...
Dan/drbwoodworks

Soft maple and have used hard maple a few times . We make our doors and can't remember ever having a door warp . We always prime the panels with a tinted primer that matches top coat . If you're spraying lacquer the finish is much better than poplar . I think poplar dents way easier too.

8/27/16       #11: What species of wood are you using ...
Harold morantz

Website: http://morantz cabinets.com

There is an interesting thread in the knowledge forum about the advantages of MDF one piece doors. They are all we use and once finished with a high quality conversion lacquer, they are as good or better than a 5 piece door. We band the square edge shakers with maple or birch banding and our finisher takes it from there.


View higher quality, full size image (2272 X 1704)


View higher quality, full size image (1434 X 1920)

8/28/16       #12: What species of wood are you using ...
Scott

The doors look ok in the picture, are the huge spaces above the pull outs there for a reason?

8/29/16       #13: What species of wood are you using ...
Harold morantz

Website: http://morantzcsbinets.com

Our standard is 3mm. The dishwasher looks like it may have been installed a little low and had a larger gap. Expanding a photo on phone or computer always makes these gaps bigger than they are.

8/31/16       #14: What species of wood are you using ...
Adam

Soft maple with glued in mdf panels.

Poplar used to grow like a weed. Now with all the extra CO2 it grows as fast as bamboo with some trees having 1 inch growth rings.

It was a poor wood for anything but trim. Now its getting dodgy for even trim. I haven't trusted it for doors for 20yrs.

I think the only thing growing faster than poplar is the poison ivy vines. Isn't climate change great...

9/3/16       #15: What species of wood are you using ...
Larry

Soft maple

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello