Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Any idea what could cause this 3 years later?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Any idea what could cause this 3 years later?

2/28/19       
Chris

Solid poplar 4/4 BTW.


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (4032 X 3024)

2/28/19       #2: Any idea what could cause this 3 ye ...
Larry Schweitzer

W/O more information I'll have to do some guessing. The moisture content of the poplar changed from when it was fabricated. Therefore it changed size. If provision had not been made, during it's original fabrication for movement, something had to give.

2/28/19       #3: Any idea what could cause this 3 ye ...
rich c.

High heat, low humidity, no accommodation for the wood to shrink.

2/28/19       #4: Any idea what could cause this 3 ye ...
Chris

lesson learned...use ply. At 4 1/2" wide, I wouldn't have thought. This happened 3 years after it was installed BTW.

2/28/19       #5: Any idea what could cause this 3 ye ...
Leo G Member

The band trim was glued to the header which has the grain going it the opposite direction. When the humidity changed the header couldn't move and instead split.

3/1/19       #6: Any idea what could cause this 3 ye ...
rich c.

To quote the Big Lebowski, "Sometimes you eat the "bar", and sometimes the "bar" eats you." Sometimes you get away with cheating rules of wood movement for a while, most times it comes back to bite you.

3/1/19       #7: Any idea what could cause this 3 ye ...
Leo G Member

HI have a 22" wide curly maple tabletop that I glued breadboard ends onto it. It's been that way since 1990. Knock on wood.

3/1/19       #8: Any idea what could cause this 3 ye ...
Dave Sochar Member

3 years, hmmm. The day before I saw this, I would think the practice of cross grain gluing a 4-1/2" pc of Poplar was fine. Then the phone rings "The Mantel is falling apart!" I think it is mantel. If so, and used on what we used to call a fireplace, it could have overheated and stressed the wood.

So, yes, refine your process. Rethink Poplar - almost any wood is better for movement. Soft Maple has become the standard wood for our paint grade interior work. I think if you had coated the end grain of that Poplar with yellow glue where the band crosses it, you would still feel ok about the 4-1/2" in a cross grain situation.

Now, take a look at our doors and you will see large bottom rails up to 10" wide or even wider and you will see a huge potential for cross grain movement. But, those big rails don't move. They don't crack. The reason? I feel it is the species - Honduras Mahogany or rift White Oak - and the construction - real mortise and tenon with coped and stuck profiling, all glued under pressure.

So, there are ways to do what you did and call it good practice. But that combination of Poplar, no restraint other than the band, and heat - perhaps a single overheated event - all conspired to cause that split.

3/1/19       #9: Any idea what could cause this 3 ye ...
Jonathan Mahnken

Fill it and touch it up. It might be stable by now. If not use a more flexible finish for this one. It probably would have helped to prime the back side. it is also possible that the affected area was an end cut, or near to an end of the original board where there was already a fracture from the drying process.Next time use plywood or laminated lumber for that width.

3/1/19       #10: Any idea what could cause this 3 ye ...
Leo G Member

It's 4 1/2". I don't think plywood is necessary for that narrow a width. If he said a whole houseful of trim started doing this shortly after it was installed then there's an issue. This is 3+ years later on a single casing. Chit happens. Repair it best you can and call it a day.

3/1/19       #11: Any idea what could cause this 3 ye ...
Gerry

I find poplar moves a lot more than soft maple. I tried poplar for passage doors for a short while and went back to soft maple for paint grade.

3/2/19       #12: Any idea what could cause this 3 ye ...
KCR

It's also possible that this end of the lumber used was close to the end of the board you used and all the end checking from kiln drying wasn't cut out before assembly. As a result the crack just continued to grow more over time. When cutting off mill-ends I always take a little more off than I would like just to be sure I get out all the end checking. Then flex the scrap end to see if it breaks. If it does I take off a little more again.

3/2/19       #13: Any idea what could cause this 3 ye ...
KCR

Oops! Johnathan said that already, sorry, didn't read everything.

3/3/19       #14: Any idea what could cause this 3 ye ...
Pat Gilbert

MC is most likely the problem, I doubt heat is the problem.

Did this occur in the winter time?

3/4/19       #15: Any idea what could cause this 3 ye ...
matt

I agree with Leo G. It does look like the split stile is glued to the header as well as the side piece, and as it shrank, it wasn't able.... thus the cracks form.

I've seen similar cracking on wide door trim with a backband around it. If done by an experienced trim carpenter, it's only nailed on with brads and a little caulk after the first coat of paint to hide the joint. If it's done by a rookie, they glue the hell out of it, and it starts splitting once the winter dry hits.

3/26/19       #16: Any idea what could cause this 3 ye ...
Chris

Thanks fellas.
Im beginning to hate solid wood. Maybe we just use mdf crossband ply or mdf for anything over 2.5" wide where everything is glued together. Coping/mortises etc is just too time consuming in my opinion. 25 years in and still learning. It disturbes me that sometimes things that shouldn't work do (like laminating one side of a huge panel and it stays flat for 10 plus years... and things that should work, dont...like laminating both sides of a panel with the same lamination and it warps in 3 days. Perhaps I need to put my science hat on.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello