Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: veneer problems

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

veneer problems

9/25/19       
the google Member

it has been a couple years since i last veneered but i'm having problems getting corners to stick.

vacuum bagging. -18 - -21 pressure (auto cycling). walnut (wood-on-wood) veneer going over solid walnut (test piece) and baltic birch. 80 g scuff both the substrate and veneer. better bond x press glue (purchase 2 months ago). using their glue spreader/roller to apply to the substrate only. bagging it for an hour (per directions on glue bottle). using top and bottom cauls.

it seems to stick fine in the field but not at the corners. we get glue squeeze out everywhere and are spreading it to touch all surfaces on the substrate. peeling it back makes it seem like we missed gluing the corners but this isn't the case. you can see the squeeze out all around the corners.

thoughts?


View higher quality, full size image (2250 X 3000)

9/25/19       #2: veneer problems ...
Tom Gardiner

I think you have too large or an overhang on your cauls. This effectively cantilevers over the edge and causes glue bond problems when vacuum veneering. Aim for a 1/4" or so. I am not familiar with the glue but it appears from your photo to be glue starved at the edges and too much back from the edge.

9/25/19       #3: veneer problems ...
TonyF

the google:

Perhaps just because I do it differently, but I cut the substrate oversize to what I need as a finished size, and cut the veneer and the caul (in my case, a piece of 1/8" masonite) to the same size as the substrate. I also only press one side at a time, that side being against the membrane material of the press.

If the caul was larger than the substrate, the force of the press may have caused it to buckle past the substrate, lifting it off the edge of the substrate, which would leave the area at the edge of the substrate with less pressure on it, and the pressure on the rest of the caul would remain once the buckle had straightened out over the center of the piece. This may have even been the case with just the veneer being oversize, as shown in your photo.

I had this happen to me years ago on a time consuming sketch face that I taped up, and was heartbroken when that happened. I have pressed a lot of veneer in the manner I described since then, and have had no issues.

Hope this helps.
TonyF

9/25/19       #4: veneer problems ...
the google Member

thanks for the ideas.

i'll have to double-check things tomorrow but i'm pretty sure we're getting on both side. top and bottom cauls are 3/4" melamine. top caul was 3/4" over-sized on all sides. we reduced this to 1/2" on our latest test.

with veneering one side at a time - i really didn't think this was possible to do without affecting the flatness of the substrate. i'd much prefer to do this for the table glue up (4x7.5 x 2 pieces). what would be the procedure?

9/26/19       #5: veneer problems ...
TonyF

the google:

For flat work I made a frame press that will accommodate a 4x8 sheet; I would veneer the bottom of a table, and then veneer the top shortly afterwards on the same day. My vacuum pump runs constant and is set on a timer for 3 hours. I use Franklin Cold Press glue (similar to the Better Bond) and a much thinner caul (1/8" masonite); if the veneer is pourous I will place wax paper between the veneer and the caul, but I veneer directly without a crossband, so this would not be a problem for you in this application.

So far, this has not been an issue for me, and I have pressed a variety of veneers including burls, some that I have flattened myself.

Perhaps others will weigh in, but what jumps out at me is the thickness and rigidity of the cauls, as I think the idea is to draw the veneer down to the substrate, and the rigidity of 3/4" melamine might not pull down tight against the veneer, and unless everything makes contact everywhere, there will be areas that have no pressure applied to the veneer. This is also why I veneer one side at a time, as the rigidity of the substrate may replicate this condition on the bottom veneer as well, if you are veneering top and bottom in one pressing.

As I have no formal veneer training, but instead lots of trial and some error, others may well disagree with what I am saying, and weigh in with their view and experience.

Just trying to be helpful.
TonyF

9/26/19       #6: veneer problems ...
the google Member

tony - thanks for your reply. i appreciate you sharing your approach and suggestions. my lead guy is out today but i'm planning on testing some sample pieces out shortly.

we seem to get getting a slightly better bond at the corners on the bottom side than the top side but all are still not as good as the sides. our test piece caul was maybe too big and provided too great an overhang.

with you putting your veneered side down - does it really matter about the caul? i would think the caul, and don't top and bottom sides at one time, would matter, but be irrelevant if only veneering the bottom side in one pressing.

9/26/19       #7: veneer problems ...
TonyF

the google:

Perhaps I did not state it clearly.

The face that gets veneered, whether it is the back or the front of the panel, is always face up in my press, such that there is the substrate, the glue, the veneer, and the caul, and that is face up against the membrane that is being sucked down onto the face being glued. In this manner, the vacuum only needs to overcome the resistance of the veneer and the 1/8" caul, and can provide maximum consistent pressure to the face being glued.

Perhaps the confusion was in stating that I glued the bottom and then the top of a table. The bottom face of a tabletop would be glued first, face up, in the manner described above. After that was dry, I would flip it over and do the top face of the tabletop, face up, in the manner described above. Both faces would be glued on the same day, so that it manages to stabilize the substrate and minimizes any warpage.

TonyF

9/27/19       #8: veneer problems ...
Tom Gardiner

One other thing. With adhesives more is not better when veneering. Excess glue may lead to extended cure times, bleed through marring the surface, and too much squeeze out will gum up tooling. I aim for just barely opaque glue surface and small - less than 1mm beads of glue squeeze out.

9/28/19       #9: veneer problems ...
Larry Schweitzer Member

We pretty much do the same as TonyF. We have a 5 X 10 vacuum table that is very flat, has grooves in the bed. A hinged frame with the membrane. Much easier to use than the bags we started with. We also use 1/8" hard board cut very close to the work size. In the press less than one hour, flip and do front side. Our membrane is urethane, wish it was silicone so we could contour press solid surface w/o some form of insulation.

10/7/19       #10: veneer problems ...
Pinetree

Google

I know you said the directions said an hour for glue up but that sound short to me . Also are you meeting your open time because you can get dry edge if the open time is really short. I use cold press from franklin and had that happen because dry edge. I press for 2-3 hour depending on conditions and open time is 15 -20 min. Try a differant glue because it sounds like everything else is fine .

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello