Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: help buying a new edgebander

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

help buying a new edgebander

8/18/17       
danny collier Member

looking at the Holzher 1327 and the SCM k560 both are servo. has anyone had issues with the servo motors? Any issues with the computer and or software? Is using the PUR glue worth it? Is one bander better than the other?

8/18/17       #2: help buying a new edgebander ...
bruce Member

we have the holzher 1329 and the scm k600 which both are a little over a year old.
we use the holzher with pur glue only as to apply laminate edgebanding since laminate can be troublesome to apply with eva glue without priming the laminate strips first .
we use the scm with eva glue to apply pvc edgebanding only.
Both machines have been great so far and we run them hard for 9 hours a day .
the scm works better for pvc banding and the holzher works better for laminate edges for us.
we've had no real issues with either machine .
What edges are you gonna apply or both?

8/19/17       #3: help buying a new edgebander ...
danny collier Member

we will be doing mostly pvc and wood strips. verry little laminte. some 3m. have you used your holzher for pvc? you say the scm does a better job with pvc, but how much better as i am now more inclined to go with the holzher as i have had discussions with techs and owners of the holzher who swear by it.

8/20/17       #4: help buying a new edgebander ...
bruce Member

Concerning your thoughts on pur glue..since you be running very little laminate then I would stay with eva glue without a doubt. Pur glue and cleaner can get expensive and cost of labor and such for clean up ..
Yes we have and do run a little bit of pvc on the holzher and it does a great job.. What I meant was the way we run our shop.
Are you going with all servo motors on each station? Just make sure the tech goes over and gets you to totally and completly understand how to adjust each station with the on-screen menu.
If you go with a glue pot machine then bite the bullet and buy a extra glue pot.
I think you would be satisfied with either machine..

8/21/17       #5: help buying a new edgebander ...
danny collier Member

to bruce..do you have any servo motors on either bander? my concern is the accuracy and future reliability of the servo motors as i hear they are very costly to replace

8/21/17       #6: help buying a new edgebander ...
bruce Member

jut 1 motor on our scmi which adjusts the pre-mill fence. everything else is manually adjusted . our holzher has quit a few as most stations are adjusted on screen.. we have had zero problems out of them. accuracy is great. where are u located?

8/25/21       #7: help buying a new edgebander ...
Ryan

Website: http://patzerwoodworking.com

We currently have a 6 year old Hozher 1336 Arcus and we run PUR on everything. We are 70/30 commerical to residential cabinetry and we found that the PUR made sense for us. We run 3mm and .018 PVC almost every day and have great success with it. We do try to buy 3mm FLEX banding as it has less memory than the rigid and gives the PUR time to cure. We have had several SCM banders and every once in a while we had issues with banding falling off and problems with the glue pots, so we decided to make the switch to Holzher entirely because of the PUR. Of course we have had our issues, but I haven't had 1 call in 6 years about a band falling off and thats a big deal when you are delivering product up to 6 hours away.
We just ordered a new 1556 Accura that will be here end of the year and they have made some nice changes.

6/22/23       #8: help buying a new edgebander ...
Allen Slotto Member

Our shop bought a k560 2 1/2 years ago. To be honest, we have fought with the adjustments ever since. At install, the tech literally said "I know what the numbers need to be, so I can't help you with that, you'll just need to play with it and figure it out". And yes, that was what he told us almost word for word. Finally, talking to a different tech who admits he isn't very familiar with the all servo machines, he told us how to get the machine adjusted properly. We spent 1 1/2 days getting it adjusted after that, cutters, scrapers, we had it set quite well, but then a crash a week later... If anyone can help, we think the crash has perhaps caused the top scraper to not be in position now, but we can't find any reference where to physically mount the scraper within range of the base setting for .5mm banding. 1mm and 3mm seem to be working properly, so we are confused why the scraper is not even close to the board with .5mm banding. I know, this isn't really an answer to your original question, but I mean it to be an insight to the need to force the tech to do his job and explain these adjustments. Our primary problem was that the tooling base setting was not within the adjustment range for the user profile. Now finally we are closer, but still again a little off

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • American Fabric Filter Co.
      Provider of Custom Made Filter Bags and Transfer Sleeves
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • WoodJobs.com Search Consultants
      Free Employment Service for Woodworking Related Job Seekers
    • Sandman Products
      Affordable Sanding Tables and Inspection Lighting
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • The Millwork Studio
      Millwork Shop Drawings and Estimates
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!