Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Curved cabinet top

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Curved cabinet top

5/24/23       
Dave Wildman

Hi

I am making a built in cabinet with a arched top. It will be going into an alcove so only the face and interior of the cabinet will be visible. It is going to be frameless but will be shimmed and have an applied casing which can help keep the front from flexing and it will have a 1/2" back. Radius for the arch is approx 30". My plan is to cnc the forms for the inside radius. Its too big to go in my vac. bag so my thought is just to use a bunch of ratches straps. I plan on using 2 layers of 3/8" bendy ply and then a veneer layer inside and out. (outside won't be seen). Is this enough layers or should I plan on using 3 layers of the bendy ply? I was just thinking titebond for the layers but could use urea resin to help increase the stiffness. I will be using 20 mil backed veneer for the face. Thanks!

5/24/23       #2: Curved cabinet top ...
Leo G Member

Kerfcore. Veneer both sides to maintain it's shape.

Kerfcore

5/24/23       #3: Curved cabinet top ...
Dave Wildman

Leo. Thanks. Would you suggest 2 layers of kerfkore and then the veneer. I have no framework to attach the kerfkore to so it will need to be self supporting. I think I have seen a video where the kerf sides are laminated together resulting in a rigid curve. Is that what you would suggest?

Thanks

5/24/23       #4: Curved cabinet top ...
Leo G Member

It gets pretty rigid if you put a veneer on both sides. On the unseen side you can probably use a polybacker.

I've used it for making curved cabinets. In that case I used a curved rib that I nest into a groove and glue to have it retain it's shape.

5/25/23       #5: Curved cabinet top ...
Tom Gardiner

I think you should use two layers of 3/8" bendable ply with veneer on the exterior surfaces. Make a disposable vacuum bag from heavy vapour barrier and butyl tape. Bag up your layers and clamp the bag to your form. Ratchet straps alone won't give the distributed clamping pressure for a successful glue-up. You can google home made vacuum bags to see the set-up.

5/25/23       #6: Curved cabinet top ...
Bill

I agree with Tom.

5/25/23       #7: Curved cabinet top ...
Dave Wildman

Leo. Thanks.

Tom. I think I will give that a try. Would titebond be an acceptable glue or would you suggest a Urea resin or epoxy glue?

Thanks

5/26/23       #8: Curved cabinet top ...
Pat Gilbert Member

You will have less spring back with plastic resin glue

5/26/23       #9: Curved cabinet top ...
Thomas Gardiner

I press almost exclusively with PVA. Call me stubborn or cheap but I rarely have a glue problem. Spring back may be more with PVA but it won't be and issue with this application when the top is fixed to the gable and back. Choose your glue based on your experience with veneer. Are you confident that you will get the layup in the bag, clamped to the form and drawn down to vacuum before the glue starts to set. If you are using raw veneer will it buckle too much.
PPR will give you a longer open time, I'm not sure if it has less moisture though.

5/26/23       #10: Curved cabinet top ...
Bill

Based on my experience I agree with Tom.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • American Fabric Filter Co.
      Provider of Custom Made Filter Bags and Transfer Sleeves
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • WoodJobs.com Search Consultants
      Free Employment Service for Woodworking Related Job Seekers
    • Sandman Products
      Affordable Sanding Tables and Inspection Lighting
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • The Millwork Studio
      Millwork Shop Drawings and Estimates
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!