Solid wood drawers

11/29/18       
Willem Martins  Member

Website: thelastwoodworker.com

For solid wood drawer sides and ends, do you make your own, or do you buy dimensioned lumber?

If you make your own, plane or re-saw?

11/29/18       #2: Solid wood drawers ...
Dustin orth

Website: http://customwoodmontrose.com

We use all solid soft maple at 5/8 thick. All dovetailed in house. All material comes in at 15/16, yielded out on the straight line rip, glued up to maximize sizes then run thru the moulder to get down to thickness. All drawers less than 9" go that way, bigger will go thru the planer, then all get finished in the widebelt. All stock is then racked until it's needed. We generally use only 4 sizes for both rollouts and drawers so that makes stock levels easy to see and decide how much to bring in.

11/29/18       #3: Solid wood drawers ...
Ryan

How can one make one building and finishing solid wood dovetail boxes when places like hardware resources sell them so cheap? We would need one if not 2 more guys to keep up with the number of drawers that we buy and thats a lot to add to payroll.

11/29/18       #4: Solid wood drawers ...
Dustin orth

Since we make all high end custom and have the tooling and employees that can make our drawers in house we will continue to do so. Our normal kitchen or house job has around 50 drawers and only takes us around 3 to 4 man days it makes sense to keep it in house.

11/29/18       #5: Solid wood drawers ...
Ken Member

Simple Ryan, cost analyses. How much are 50 boxes from Hardware Resources vs cost of man hours to produce in house. It may not make sense for a 1 or 2 man shop with manual machines but if you have the equipment it may.

11/29/18       #6: Solid wood drawers ...
Willem Martins  Member

Website: thelastwoodworker.com

I also make all my own drawer boxes. I can beat prefab box prices every day.

Current kitchen Beech drawer boxes with pre finished Maple ply bottoms.

We got a bunch of Beech at an auction, getting 14mm out of resawing two per board.

I believe if set up properly, it is well worthwhile doing in-house.

11/30/18       #7: Solid wood drawers ...
Ryan

So are y'all prefinishing the stock and then cutting to length and running it through the dovetailer? I know that you can get a dovetail machine in the 15-20k range which isn't all that bad.
Then my question comes in Dustin if you have 3-4 days in 50 boxes then 24-32 hours. Which if my math is right is $37-$41 labor in a box if your shop rate is $65 (in my area thats a good average) an hour. On average over 50 boxes I am paying right at $40 a box for solid 5/8 maple dovetail boxes delivered to my door.

11/30/18       #8: Solid wood drawers ...
Ryan

I don't want my last post to sound like I am coming off rude. I am just trying to think through the cost of doing it.

I can see where is makes since if you are trying to get them in a quicker time frame as it normally takes 2-2.5 weeks from the time we order to get them.

When we run into a small job which isn't normall for us. We normally work in very high end 7,000 plus sqft. homes in a lake community. We will run it by the customer and if they want their cabinet quicker than we can get the boxes in then we will cut prefinished on the cnc and edge band the tops on the boxes.

11/30/18       #9: Solid wood drawers ...
Dustin orth

Website: http://customwoodmontrose.com

The material is not prefinished on the rack. We cut the ready blanks to length, dovetail, assemble, sand and fill voids then spray . With where we are located the shipping costs are not good compared to building in house. We also use wormy maple for the material, our customers really like it, most suppliers charge a premium for that yet we don't pay a premium for the raw stock, less than anything else comparable. Plus I don't have to wait 2 weeks for a drawer order.

11/30/18       #10: Solid wood drawers ...
JeffM

I haven't found a drawer box company yet that is cost efficient built the way I want them and shipped. For me to build one, material is less than $5 per box and labor is minimal. I get my material 13/16", run though the planer one time to 11/16 and run through wide belt. Cut grooves for bottoms on TS then finish the insides. Dovetail all around (faster than dadoing the back) and assemble with glue and pins (no real need to clamp the boxes). Rout the top edge...sand and finish.

11/30/18       #11: Solid wood drawers ...
Hen Bob Member

For the guys building them in house, in real time how long does it take to finish the drawer? I would think two coats would be necessary to get a smooth surface be it solvent or WB

11/30/18       #12: Solid wood drawers ...
MarkB Member

Im in Jeff's camp. We buy hard maple s2s SLR1e for cheap. 15/16 plane to thickness, dovetail, and ply bottoms. Dont know about others but our jobs usually have a fair amount of deep pots/pans drawers and I have never had my average number for a job worth of drawers that we've sent out to bid come back a 50 bucks a drawer average. Maybe for shallow silverware drawers but when you start getting into a lot of 6", 9", and deeper, drawers the numbers go way up. We have a good bit less than $10 total in materials in a large box that would probably come in at $100 bucks to bring in including freight. If we cant build a box in-house for $90 bucks after materials we have no business being in business.

I can easily see in a large operation production cabs where your covered up with work outsourcing stuff like this all day long. Our customers however pay a bit more and they have walked out of the shops that outsource everything they touch. They ask specifically what "we" make, and are also interested in the fact that the hardwood in our work comes from entirely within the state.

11/30/18       #13: Solid wood drawers ...
JeffM

Hen Bob.
I can finish all of the insides of my drawer pieces in about an hour. After assembly, I can finish the exteriors in 2-3 hours including dry time and sponge sanding. One sealer coat and a double full coat...meaning i spray it twice but while the first coat is still somewhat wet. I guess you could call it 3 coats.

11/30/18       #14: Solid wood drawers ...
Hen Bob Member

I absolutely get the material cost aspect of doing them in house, our bottleneck is finishing, and the time of moving them around for drying, scuff sanding etc.. drawers take more room than a vertical rack of doors. Our labor rate is higher due to location and overhead.

11/30/18       #15: Solid wood drawers ...
Leo G Member

I agree with MarkB about the non average drawer. The top line of drawers in a kitchen, ie: 4" tall drawers, are relatively inexpensive to order. But as soon as you get into tall drawers the price skyrockets. I basically build my drawers with Baltic Birch plywood which makes material processing a cinch. I have a manual dovetail machine. As long as the drawer is less than 8" it's two passes per box. Taller than that and I have to do each corner separately.

12/2/18       #16: Solid wood drawers ...
Adam

We do it all of those ways.

Order them when we are busy and can work around the manufacturing/shipping times. As others have noted the big ones are expensive for them to make and ship.

We've got drawer company within an hour who make good cheap drawers. We often use them for wardrobes, vanities.

Most kitchens we've made in 15 years always have huge drawers for this and that. As well as some "interesting" designed drawer liners. We do a lot of library/studies. Likewise these are not typical drawers.

As far as materials. Depending on the project we will use hard white maple or baltic birch. Customer typically makes the call based on cost.

Our finish is MLC wb Agualente. Its got this really cool waxy finish. 2 coats gets the job done. They don't smell like CV or laquer for the next month.

12/3/18       #17: Solid wood drawers ...
Mark Member

Mark B,

I think you need to go back and look at your numbers.

A large box can easily have 8 1/2 sq ft of material, so depending on your yield, you'll need to add to that number. Now factor in the sq footage for your ply bottom and you're closer to $20-22.

1&2 White hard maple is still over $2 bd ft, especially with the spec you are bringing it in at.

12/4/18       #18: Solid wood drawers ...
MarkB Member

A little low but not by much but of course the size of the box your ballparking has everything to do with it. We dont pay anywhere near $2 a foot for the hard Maple we use on drawer boxes. The last unit we brought in was #1 common, S2S SLR1E-15/16-stain and we pay about $0.88/BF for it. By the time its down to draw box material its clean no-stain. A 7x24x21 box figuring way high is about 5.5BDft figuring taking if from 8" material and an extra half a foot for waste which is ridiculously high puts you at 4.84. Another $6-7 for a domestic bottom, more like $4 if we were running import.

12/4/18       #19: Solid wood drawers ...
MarkB Member

Mark,

So now Ive given you my rough numbers, so what are your specific numbers for a 7x24x21 box, materials only, and then what would that box cost you to buy in raw, flat?

12/4/18       #20: Solid wood drawers ...
Mark Member

Mark B,

1C 1&2 White is running $1.60 bd delivered ft in full units. SEL & BET stain is $1.70 delivered. Never priced 1C stain.

7 x 24 x 21" $47 finished and assembled in white HM is what I sell that box for.

Mark

12/5/18       #21: Solid wood drawers ...
MarkB Member

As a drawer manufacturer? $47 fully assembled, clear finish, plus shipping?

12/5/18       #22: Solid wood drawers ...
Mark Member

Mark B

Yes, I'm a regional manufacturer and have never pursued out of state business.

The reality of drawer boxes is that every major metropolitan area can support an operation like mine.

Before you ask, I'm in Pontiac MI

Mark

12/8/18       #23: Solid wood drawers ...
Daniel P Member

I get my drawers from Hardware Resource my only gripe with them is they use very little glue in their joints. I got a order once and the joints were coming apart when I got them I had to reglue some. I did call them and complained for what little good that did.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello