curved kitchen curved doors

8/21/21       
michael foster Member

I have to build a kitchen with curved faces in 3 sections of the cabinets. 2 of the curves are concave and have a radii of 14' and 10' 2". The other is convex with a radii 8' 2". The drawers fronts and doors are to be built of 1/4 sawn mahogany they are only 2 upper doors curved all of the rest are curved drawer fronts . The grain of the wood is to run horizontally. The doors are flush no panel or frame. The fridge has a curved panel for the doors. The main stipulation on the job is that it must be made of all local material and Barbados does not manufacture plywood. I could laminate my own ply once it is made from local material. How should I go about building these panels

8/21/21       #2: curved kitchen curved doors ...
Tom Gardiner

Does Barbados have a veneer mill? If not I suggest resawing solid into veneers of a thickness that will bend easily to the radii desired. The amount of springback is determined by the number of plies (a lamination of three 6mm plies will spring back much more than six of 3mm)
This will take care of the drawer fronts but not the fridge panels or doors. If you are stuck using solid for the job, you can cooper together curved door cores from solid staves - beveled sticks. Then you would smooth the inside and outside faces and veneer across the grain. You have the advantage of a more consistent humidity in the Caribbean as opposed to Canada and mahogany is very stable so the chances of this approach working is much higher than if I were to attempt it.
A vacuum veneer set up is pretty much a necessity for these techniques. You will need to make forms for each radius that will account for springback.

8/22/21       #3: curved kitchen curved doors ...
cabinetmaker

Cooper the doors and use on a jig to clean up the radius inside and out taking very light passes. Use a good soft pad on a random orbit sander with no more that 120 to start and take your time.

Seal and finish both sides, fill end grain well and seal like the front and back

8/22/21       #4: curved kitchen curved doors ...
michael foster Member

Thanks for the information so far.
It seems I should get full information on either
(1) making veneer and gluing up sheets of the veneer possibly using a vacuum process with molds offset to correct kickback or
(2)building a thick enough flat Panel out of solid wood staves And cutting the front and the back into the required curve with some kind of jig and a router.
After I am clear what is involved in both I can decide which route to take.
Is the second option at all possible and if so can someone describe to me how it is done.
For the drawer faces that are curved out in particular it may make sense to cut the front of the face into a curve and leave the back flat to affix to the drawer box.
Looking forward to your expertise
Michael from Barbados.

8/22/21       #5: curved kitchen curved doors ...
michael foster Member

remember the grain is running horizontal and the face looking at a floor plan is curved.

8/22/21       #6: curved kitchen curved doors ...
michael foster Member

Sorry to clarify I wrote in my second post that I could use thick enough wood staves that was in correct I meant thick enough square edged pieces of wood may be 1.5"x3" by the width of the drawer face.
Michael.

8/22/21       #7: curved kitchen curved doors ...
Tom Gardiner

In my opinion, for the the doors and fridge panels, the coopered core will have to have the grain running vertically (quartered stock). After fairing the curve then you will have to veneer across the grain to get your horizontal oriented grain pattern.
Your fridge panels and the drawer fronts can have flat backs which makes life easier. The drawer fronts may be bandsawn from thick stock to the face radius sort of. I would recommend veneering the face and back to avoid the ugly transition to end grain.
The evil side of me is asking how would the client know that sliced veneer was not local. There is a ton of labour and waste involved in shop sawing your own veneers. Commercially available veneer is so good and convenient.

8/22/21       #8: curved kitchen curved doors ...
pat gilbert

The curves can be made with a stroke sander or a planer, have the knives ground to the curve you need, or a William and Hussey

If you can veneer use plastic resin glue to avoid spring back

8/22/21       #9: curved kitchen curved doors ...
michael foster Member

Tom
I don't understand
to avoid the transition to the ugly end grain.
I think I am misunderstanding the process you are describing.

8/22/21       #10: curved kitchen curved doors ...
Tom Gardiner

If you were to use a solid block of 8/4 mahogany to make your drawer fronts by just band sawing the front curve you would end up with flat grain figure just in the centre of the front. As the curve moves towards the ends of the drawer front it will cut on an angle to the grain direction. This tends to suck up stain and finish in a blotchy unpleasant look.

8/22/21       #11: curved kitchen curved doors ...
michael foster Member

Thank you Tom.
I am trying to have the face showing end grain.
I have veneered a kitchen but I have never made any veneer. I have to do some to scale sketches to see how thick a wood these varius curves and width doors would require.

8/23/21       #12: curved kitchen curved doors ...
michael foster Member

If I build curved panels with staves how can I cut the edges to make a smooth curve. Ive seen it done with a cnc machine but I have no access to one.

8/24/21       #13: curved kitchen curved doors ...
pat sgilbert

You could sub the doors out

8/24/21       #14: curved kitchen curved doors ...
cabinetmaker

You will be glueing up
a segmented shape. Think octagon

Knock off the hi spot with a hand planer, belt sander or router on a trammel a lot like a lathe.

Then just fair it with a good strong random orbit sander

8/24/21       #15: curved kitchen curved doors ...
michael foster Member

You lost me at
"use a router on a trammel a lot like a lathe."
I'm not sure what a trammel is. So getting a trammel and a router to work a lot like a lathe is even more confusing.
Would you give me a clearer explanation?

Michael

8/24/21       #16: curved kitchen curved doors ...
michael foster Member

The Question in the previous post I made, is a question for cabinetmaker

8/25/21       #17: curved kitchen curved doors ...
cabinetmaker

see link below

this is a sled design and it would be pretty easy to do

https://hu.pinterest.com/pin/367958232027604899/


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • American Fabric Filter Co.
      Provider of Custom Made Filter Bags and Transfer Sleeves
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • WoodJobs.com Search Consultants
      Free Employment Service for Woodworking Related Job Seekers
    • Sandman Products
      Affordable Sanding Tables and Inspection Lighting
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • The Millwork Studio
      Millwork Shop Drawings and Estimates
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!