CNC drill through HPL

5/27/22       
BEN ROBINSON Member

Hello there,
I have gotten loads of information from the site and thought I would try my luck with my question. We manufacture casework commercially. I am trying to get set up to route my doors and drawer fronts on my CNC.
The problem I am running into is the 3/4" lock hole. I cant get a clean cut on the bottom side (the outside of the cabinet). I have worked at other places that have achieved it, but just cant get the right settings to work with me. I have tried a couple different 3/4" bits, but not working out that well. What have you all done to help achieve a good through hole? Slower speeds? Slower feed rates? Higher feed rates? Thanks!

5/27/22       #2: CNC drill through HPL ...
Mark B

I dont know about 3/4" but with smaller holes if Im trying to get a really clean hole (no blow out on the bottom/show face) I run brad point and I set my depths so the knickers on the brad point just barely come short of cutting through the HPL face. This most often leaves a small hole in the center and a the perimeter of the hole barely cut through the HPL and it just pops out when the sheet comes off. Punching through, even with a fresh spoil board, will typically blow out most every time.

With a 3/4" hole why not just waste away the material with an interpolated hole and a smaller tool and skip the drilling? Its not as fast but with so little cover on a lock you'd get every hole bang on.

5/27/22       #3: CNC drill through HPL ...
RichC

I'd suggest a 3/8" uncut spiral router bit in a spiral down program that starts in the middle and then moves out to the outside diameter instead of a drill bit. A light finishing cut wouldn't hurt either.
If you insist using a drill bit, do a pecking cut with the final breakout being a VERY light cut

5/27/22       #4: CNC drill through HPL ...
Mark B

Any tool in the changer, even a half inch compression with an interpolated hole would work. The issue is the drill block is faster but getting a show face hole clean enough for the lock would be a bear. A single (or couple) blown out holes would put me in the interpolated column in short order.

5/27/22       #5: CNC drill through HPL ...
Dropout Member

Don't like drilling with a router bit. Hard on everything.

Drill the hole first with a 1/2 v point bit and then use a compression spiral to open up the hole to the diameter you need.

Little more time but always perfect.

5/27/22       #7: CNC drill through HPL ...
BEN ROBINSON Member

Thanks alls,
I am running AI center, with RouterCAD producing the G-Code. I have a couple of sample holes that I will try in a few minutes. I will try all the different size bits in the interpolated. I wasn't sure how to make my program do that type of hole, but figured it out!

5/27/22       #8: CNC drill through HPL ...
Mark B

Not to argue with Dropout but an interpolated hole is not drilling with a "router bit". High plunge rate spiral interpolation (350ipm) is a basic milling cycle. Whether you run it as a pocket cycle taking the hole to diameter in two passes or one is just dependent on how your material behaves. I could easily see a 1/2" compression plunge, or 3/8" if thats whats in your changer for another op, doing a single spiral down and being dead clean.

Never be as fast as a drill but again, 1 blown hole and you've lost any time gain from the drill block.

5/27/22       #9: CNC drill through HPL ...
Dropout Member

Mark B is correct.

I tend to drill first because you can't get the feed rate high enough for a decent chip load using a 3/8 or 1/2 bit in a 3/4 hole. At least if you're just enlarging an existing hole there is less load on the tool.

Just personal preference.

Did have to tell a guy last week that "drilling" a 1/4 hole with a 1/4 down spiral bit might not be such a great idea....


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.
    Sponsors
    • Mereen-Johnson Machine Company
      Manufacturers of High Production Woodworking Machinery
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • Country Saw and Knife
      Complete Sharpening Services for Wood and Metal Saw Blades, Jointer Knives, and Bandsaw Blades
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Safety Speed Manufacturing
      Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers

    Become a Sponsor today!