RT Machine Co

CNC

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

CNC Bits Recommendation

3/25/24       
Andre Member

Hi there,

I would like to thank you in advance for taking the time to read this post and answer it.

I'm reaching out because we have been having difficulties in learning exactly what kind of bits should be used for our work.

We have a Anderson America Selexx 510 and are using this machine to cut (for now) MDF, Plywood, Particle Board and Solid Wood.

There is so much to choose, and so much information, so little time to absorb and test and not so many people wanting to share their secrets.

We do all sorts of work with this machine, specially complicated or stuff that takes a while to do by hand.

We would like to know all bits recommended, if compression bits? regular bits? which thicknesses? 2 flutes? 3 Flutes? 4 Flutes? specialized bits for each material? Specialized bits for each operation? etc

The more details included the best.

Again, I do appreciate all time taken to read this post. Any information is good information. Please if you answer try to be as much specific and straight forward as possible.

3/25/24       #2: CNC Bits Recommendation ...
cheriLongsworth Member

Website: https://wattsan.com/products/cnc-routers/

For MDF, Plywood, and Particle Board:

Compression bits: 1/2" diameter, 2 flutes
Regular bits: 1/4" diameter, 2 flutes

For Solid Wood:

Compression bits: 1/2" diameter, 2 flutes
Regular bits: 1/4" diameter, 2 flutes

Consider using specialized bits for:

Dado cutting: 1/2" diameter, 2 flutes
Groove cutting: 1/4" diameter, 2 flutes

3/25/24       #3: CNC Bits Recommendation ...
Dropout Member

Well that was pretty much a useless response.
The original question is too open ended. Kind of like "whats the weather like in the USA today?".
The answers you will get are dependent on the questions you ask.
I use 1/2 compression spiral chip breaker as short a flute as I can get, 7/8 or 1 1/8, for 3/4 plywood. Single pass, 900 IPM, no one cares about edge finish so we're probably at 3,000 plus sheets on the current bit.
At times we run 100 or sheets of ply per day.

3/25/24       #4: CNC Bits Recommendation ...
Mike

Okay,
I'm sure that didn't help you either. I would contact a tooling supplier for recommendations. You do a variety of materials and not just one type of plywood or paritcle board. Based on your horsepower on the spindle, you can go fairly fast. I would recommend getting familiar with chiploads and how to calculate them. Vortex Tool has a phone app that is pretty handy for figuring feeds/speeds/chipload for your application. The supplier wants you to be successful with the tools they sell you, so don't be shy about asking for advice. I would tell\ your what I use, but you need to learn your machine and what you can get away with as far as cut quality and tool life goes. Everybody has different variables as far as vacuum, horsepower, and machine rigidity goes. Good luck and have fun. Whether you are cutting composite material, solid hardword or aluminum, you feeds and speeds will vary quite a bit. Also how many flute the tool has. When you start to figure out chiploads, you will undertand better.

3/26/24       #5: CNC Bits Recommendation ...
BH Davis  Member

Website: http://www.bhdavis.net

I would say that to start you want to keep it as simple as possible and expand your bit collection as you learn what you are doing. I'd start with a few specific bits:

1) 2-flute carbide 3/8" upcut and downcut bits. Upcuts for when the bottom of the material needs the cleanest cut and material hold down is solid such as on panel stock, and downcut for when the top of the material is most critical and material hold down might be a bit weaker as on solid wood components.

2) 2-flute 3/8" carbide compression bit for when you need a clean surface on both the top and bottom of the material as on double sided melamine panels.

I would stay away from chip breakers and other expensive bits until you have a good handle on the basics. Early on in the learning curve bits tend to get broken with the potential to waste a lot of money.

Beyond this do as others have suggested and contact a router bit supplier for guidance.

BH Davis

3/26/24       #6: CNC Bits Recommendation ...
RichC

Volume of cutting also makes a difference. Run a couple bunks of MDF every shift and you will want to look at diamond tooling. The machine makes no difference at all in bit selection, so we don't need that constant advertisement for wattsan machines cheri.

3/26/24       #7: CNC Bits Recommendation ...
duster

If I never read another post from idiotic wattsan, it'll be too soon.

3/27/24       #8: CNC Bits Recommendation ...
Bill

We use Vortex bits. I would download their app. It can be very helpful. I would also get on the phone with them or someone like them.

Only you can judge the results you get. What is good for one operation may not be good for another.

3/27/24       #9: CNC Bits Recommendation ...
Erick Member

Website: https://virmer.com/

I don't see anything wrong with asking generalized and "stupid" questions for someone, a person is just learning

3/27/24       #10: CNC Bits Recommendation ...
Andre Member

Hi Guys,

Thank you all so very much for taking the time to answer my questions with your recommendations. It means a lot and I do really appreciate you guys always being there to answer even the stupid questions. Its the only way to learn (that and with own mistakes).

May you all have a awesome second half of your week!

PS - apologies for taking so long to answer. Been buried in work with no time to scratch it, lol.

3/27/24       #11: CNC Bits Recommendation ...
Dropout Member

It's not a matter of stupid - I say the only stupid question is the one you don't ask.

General questions get general answers.

Specific questions get specific answers is all I'm saying.

3/28/24       #12: CNC Bits Recommendation ...
Josh Koschak

Frost CNC bits, many guys are seeing much longer tool life than competitors tooling and pricing is better. frostcnctooling.com/

3/31/24       #14: CNC Bits Recommendation ...
dylan bayliss

Website: http://www.cnc-tool.com

Providing 30 years of experience we are happy to try and help you with your discovery. We represent almost every bit mfg in the industry, including Vortex. Its' always best to crawl, walk then run in this quest to maximize your production and tool life. A 4 flute "Tornado" bit or a PCD (diamond) bit is not a bit to start with as your first tool/s. (both have value, just not suitable newbies in my opinion).

Our chip load white paper link below.
https://www.cnc-tool.com/technical-white-pages.html#/

Feel free to call with any questions.
Regards
Dylan

3/31/24       #15: CNC Bits Recommendation ...
The MW Studio Sponsor - The Millwork Studio

Website: themillworkstudio.com

For your Anderson America Selexx 510, considering the range of materials you're cutting – MDF, Plywood, Particle Board, and Solid Wood – here are some suggestions:

Compression Bits vs. Regular Bits: Compression bits are excellent for reducing chip-out in laminated materials like plywood and MDF. They combine an up-cut and a down-cut flute to produce a clean top and bottom edge. Regular bits can suffice for solid wood and particle board, but compression bits are preferred for laminates.

Bit Thickness: This depends on the depth of cut you're aiming for. Generally, thicker bits provide more stability and are preferable for heavier cuts. For general-purpose work, a 1/2" diameter bit should suffice, but consider 3/4" or even 1" for more demanding tasks.

Flutes: Flutes are standard and work well for most applications. However, if you're seeking smoother finishes and faster feed rates, 3 or 4 flutes might be preferable, especially for dense materials like solid wood.

Specialized Bits: For specific materials or operations, specialized bits can significantly enhance performance. For instance: For solid wood, consider spiral up-cut bits for efficient chip removal and a clean finish. For intricate designs or fine detailing, opt for small diameter bits or specialized carving bits. For precise joinery, such as dadoes or rabbets, look into specialty bits designed for those operations.

Remember, experimentation and testing are crucial to finding the perfect combination of bits for your particular needs. Don't hesitate to reach out if you need further clarification or specific recommendations for your projects.

I hope this helps guide you in the right direction. Feel free to ask any additional questions you may have!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.
    Sponsors
    • Mereen-Johnson Machine Company
      Manufacturers of High Production Woodworking Machinery
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • Country Saw and Knife
      Complete Sharpening Services for Wood and Metal Saw Blades, Jointer Knives, and Bandsaw Blades
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Safety Speed Manufacturing
      Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers

    Become a Sponsor today!