Subject: Re: Bleaching walnut

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Bleaching walnut

4/24/24       
rich Member

Website: http://www.handmadefurniturecompany.com

I've got a project where the client's designer is asking us to bleach walnut. Its a large and thick solid wood table. I've bleach things a few times but nothing on this scale. I'm wondering how much control of the color I have with the bleaching. Does anyone have any experience doing this and if so can you provide any suggestions. Thanks

4/24/24       #2: Bleaching walnut ...
Pete

I have bleached walnut on quite a few jobs. Ive used the two part bleach. As far as control, you wont have a whole lot, if any. It just knocks the color way back so you can get the old faded antique look. I have noticed that the steamed walnut will tend to go lighter after the bleach where the non steamed walnut will remain a little darker. If it is a new table you are working on, save your cut offs for samples. If it is an existing table that you are stripping then Im not sure how well the bleach will work as Ive never done that. Either way, whenever I have to use bleach, I always explain how there isnt a whole lot of control you have with it. Always make sure you neutralize the bleach.

4/24/24       #3: Bleaching walnut ...
rich Member

Website: http://www.handmadefurniturecompany.com

thanks...its all new material...the lack of control is the concern I have. Appreciate the info.

4/24/24       #4: Bleaching walnut ...
Pete

The lack of control will only matter depending on how light they want to get the wood. A new, fresh batch of bleach will knock the color back pretty far. Older bleach doesnt work as well.

4/24/24       #5: Bleaching walnut ...
rich Member

Website: http://www.handmadefurniturecompany.com

thanks and do you have a favorite brand of bleach

4/24/24       #6: Bleaching walnut ...
Pete

I use a 2 part wood bleach. There is no name on the box. I get from a really good local paint store.

4/24/24       #7: Bleaching walnut ...
rich Member

Website: http://www.handmadefurniturecompany.com

thnx

4/24/24       #8: Bleaching walnut ...
duster

Website: http://sunvalleywoodworks.com

I made this walnut table and used a 2 part bleach on it. It was pretty easy to do, but as Pete states, you don't have a whole lot of control on how intense the bleaching ends up. Perhaps you could dilute it a bit if you were looking for a reduced bleaching effect. I would definetly do some samples on scrap. We did some samples, and noticed that the bleach was raising the grain.
Since were were looking for a smooth finish, we sponged water onto the top, let it dry overnight and the sanded it smooth again before bleaching. This seemed to help a lot.

The client loved the final result, but to me it was a desecration of $1200 worth of walnut.


View higher quality, full size image (800 X 844)

4/24/24       #9: Bleaching walnut ...
rich Member

Website: http://www.handmadefurniturecompany.com

thanks Duster

5/12/24       #10: Bleaching walnut ...
Aaron

I've done quite a lot of bleaching of walnut, and it's true you don't have a lot of control over the color (this depends of course on the composition of the wood you're starting with – hardwood v. softwood, figure and grain, etc.). One measure of control you do have is how many times you bleach the wood. In my experience 3-4 times with A/B bleach is necessary to achieve a fairly even tone, and this is also the point at which the bleaching 'maxes out.' Once the wood is completely bleached you can stain/tone to even the color further. One important step: after bleaching you should use white vinegar to stop the chemical process – this is especially important if you're only bleaching once to just lighten the wood a little.
Finally, I always sand with 320 after the bleaching process is completed. This is enough to smooth the grain back and not sand away the top layer to expose unbleached wood underneath.

6/17/24       #11: Bleaching walnut ...
Chemmy

Probably way to late to be of help, but if your having troubles, contact me, I will be pleased to help..!!

6/17/24       #12: Bleaching walnut ...
rich Member

Website: http://www.handmadefurniturecompany.com

Thanks all. Not sure where this will end up shaking out but thanks all for the suggestions and guidance.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!