Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: White Cedar for furniture making

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

White Cedar for furniture making

8/5/24       
Sean Hayden Member

Hey fellow forum readers,
I was discouraged from using White Cedar for a furniture desk bc it is not compatible with the planers, joiners, rip saws &c. too soft and there is resin. Is this true? This is the same wood that cabin log furniture is made from but I want to make nicer pieces of furniture with White Cedar.

Can this be done if the lumber is dried properly? What about Pine? Would this type of soft wood damage machines?

Thank you,
Sean

8/11/24       #2: White Cedar for furniture making ...
Dave Sochar Member

The stuff is barely wood. Extremely soft.
It was used for cabins and furnishings because it was logged to build the cabin, not because anyone desired the stuff, sought it out and brought it in to the cabin sites.
I think that today, it is used mostly for the Adirondack chairs you see everywhere.

8/13/24       #3: White Cedar for furniture making ...
duster

I've made some nice pieces using clear western red cedar and alaska yellow cedar. White cedar is just too soft for anything that is expected to last more than 2 or 3 years. I've also made a lot of pine pieces, usually with furniture grade white pine. It's soft and dents easily, so it's not great for dining tables, desks, coffee tables, ect. I have made dozens of bedroom pieces with pine and it's held up fairly well. As far as damaging machinery, I don't think that's really an issue except pine can gum up saw blades, planer and joiner knives, router bits and sanding belts.


View higher quality, full size image (800 X 940)


View higher quality, full size image (672 X 340)

9/21/24       #5: White Cedar for furniture making ...
Olmo9 Member

What specific characteristics of western red cedar and Alaska yellow cedar make them preferable choices for durable furniture compared to white cedar and pine?

11/1/24       #6: White Cedar for furniture making ...
Paisley Peacock Home Member

Hey everyone,

I wanted to weigh in on the discussion about using White Cedar for furniture, particularly for a desk. While it's true that White Cedar is softer and contains resin, it can still be used for furniture if you're careful and take some precautions.


View higher quality, full size image (690 X 410)

11/1/24       #7: White Cedar for furniture making ...
duster

WTF? I thought this was a woodworking forum, not an online retail site.

11/1/24       #8: White Cedar for furniture making ...
Dave Sochar Member

Retailers often are drunk on getting the name out. But I agree with Duster - this is no place for selling. If so, I would mention my book - Small Shop Production .......
Cedar furniture? I can imagine that bed after a few months, squeaking every time anyone moves, the bed rocking, and denting and splintering as vacuum hits it, etc.
Remember, just because you can does not mean you should.

4/24/25       #9: White Cedar for furniture making ...
Daiva Member

None of the common pines “damage” machines either. Southern yellow pine is harder, heavier, and can tax smaller lunch&#8209;box planers simply because you’re feeding denser material, but normal knives handle it.

4/28/25       #10: White Cedar for furniture making ...
David William  Member

Website: http://www.bergenfurniturenj.com/

White Cedar can be used for furniture, but it’s true that its softness and resin content may cause issues with some tools like planers and saws, especially if not dried properly. It’s best to ensure the wood is thoroughly dried to minimize resin and avoid clogging machines. Pine is a similar softwood that works well for furniture but also requires careful handling. Both can be used with the right preparation, though you may need to clean tools more often.

9/22/25       #11: White Cedar for furniture making ...
Jetrozn Member

White cedar can definitely be worked with if it’s dried right, though it is soft and can gum up blades if there’s resin. Pine is similar—sharp knives and lighter passes help a lot. It won’t ruin your machines, just means you’ll be sharpening more often. I once made a simple bench out of pine and later paired it with a sideboard I got from sicotas furniture in their Buffet Cabinets section, and the contrast of the soft wood piece next to a heavier build looked great.

9/25/25       #12: White Cedar for furniture making ...
Yash Sharma  Member

Website: https://www.woodensure.com/Side-Table

White cedar is workable, but yeah, it’s on the softer side so you’ll run into tear-out if blades aren’t sharp. Resin can be annoying, but keeping tools clean usually handles it. If it’s dried properly, you can make decent furniture out of it, though don’t expect the same durability you’d get from hardwoods.

Between cedar and pine, I’d say pine is easier for clean cuts, but both dent pretty easily. If you’re aiming for long-lasting, “finer” pieces, I’d personally lean toward a hardwood — cedar and pine are better for rustic or lighter-duty builds.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!