I'm about to start a build on a record cabinet that will have bevel slat doors and am looking for some advice/knowledge from anyone who has had experience making something similar. The doors will be solid flatsawn white oak with the slats running perpendicular to the grain. I'll be cutting the slats (1/4" deep 60 degree v-groove ) on the CNC. The doors are slab style so I won't be able to rely on a frame to help maintain flatness and account for seasonal movement. The largest door will be 16" x 18".

I'm a bit concerned about the doors warping and would like to avoid placing battens on the door interior. I have had issues with removing material from only one side of a solid wood panel in the past. Any tips? I'm not opposed to creating engineered panels (CLT, stave core or similar) but feel that 5/16" thick "veneers" are a disaster waiting to happen.


View higher quality, full size image (1162 X 971)


View higher quality, full size image (1813 X 1012)

12/17/25       #2: Bevel Slat Door Tips ...
Jr Lee  Member

Website: http://www.leecabinets.com

Isaac I have only done a similar door using MDF on my CNC but I too would be concerned about cupping/warping for the size you mentioned. I would also be concerned about the V bit splintering the material as it exits the crossgrain cut. That could easily be remedied by oversizing the doors before machining and trimming to size afterwards. Good luck
Jr

12/18/25       #3: Bevel Slat Door Tips ...
Isaac  Member

Website: http://www.milkbuilt.com

Thanks Jr. A colleague mentioned some concealed door straightening hardware from Hafele and Sugutsune that I'm looking into. They're meant for larger doors but I believe I could cut them down. Also thanks for the heads up on the splintering - I'll oversize them or use a backer to avoid this.

12/18/25       #4: Bevel Slat Door Tips ...
Tom Gardiner

Give some thought to the hinges you select. You will have a very shallow depth of material in the hinge area if you use typical euro cup hinges. Also do an expansion and shrinkage calculation to estimate how much the door height will change seasonally.
I don't envy the finish sanding you will have to soften all those edges.

1/5/26       #5: Bevel Slat Door Tips ...
Dave Sochar Member

Bevel Slat is not a meaningful phrase or description. What you are emulating is simple v-joint resulting from a tongue and groove run on reach edge of a board. The v-joint area is a 'crush' zone for expanded solid wood. The joint never looks good if it is in laminated board or plywood.

Assuming solid wood, how do you plan to accommodate wood movement?

1/15/26       #6: Bevel Slat Door Tips ...
Alex_Zhang Member

Website: https://yhcncrouter.com/

Your concern about warping caused by single-sided material removal is entirely valid. For solid wood door panels, the key is managing the internal stress balance of the wood. An often overlooked but effective method is to perform "compensatory" machining on the back side.

My specific suggestion is: After completing the V-grooves on the front using a CNC machine, mill a shallow (e.g., 0.5-1mm deep), wider relief groove on the back of the door panel, corresponding to the centerline of each V-groove, using a small straight or ball-end cutter. This serves two main purposes:

Stress balancing: Removing a small amount of material from the back helps balance the asymmetrical stress caused by the front grooving, significantly reducing the overall tendency to warp.

Providing expansion space: The shallow groove on the back provides a small "give" space for the wood to expand perpendicular to the grain, mitigating the pressure on the panel's flatness caused by expansion.

Combining this with the suggestions from other members, a complete solution sequence could be:

Material preparation: Choose thoroughly dried and stress-relieved wood. After purchasing the boards, allow them to acclimate in the workshop environment for at least a week.

Sizing strategy: Adopt Jr Lee's suggestion of processing large rough blanks and then performing final shaping.

Machining sequence: First, machine the shallow relief grooves on the back, then perform the final V-groove machining on the front.

Hardware and calculations: Carefully consider the hinge depth issue mentioned by Tom and the expansion calculations emphasized by Dave.

While this adds a few processing steps, it fundamentally improves the long-term stability of the product from a physical perspective, avoiding complete reliance on later corrective hardware.

1/16/26       #7: Bevel Slat Door Tips ...
Pete

I may be late to respond to this but I was wondering if you could approach the project with the V groove pieces as a "skin". So if your groove is 1/4" deep, mill it out of stock that is 5/16 to 3/8 thick. Id consider v grooving the back if possible to relieve stress and then glue that entire piece onto a case? Not sure if that would even work and it may need some more thought...

1/16/26       #8: Bevel Slat Door Tips ...
Isaac  Member

Website: http://www.milkbuilt.com

Thanks all. I'll take this all into consideration! The majority of each door panel will be rift/quartersawn and I'm giving myself 3/32" reveals with the max width across grain being 17.8125. Not too worried about expansion issues, just the warping. I'm going to spend the extra hour or two balancing the v-grooves on the opposing side. I'm cnc'ing it so no need to be lazy haha.

1/20/26       #9: Bevel Slat Door Tips ...
David William  Member

Website: http://www.bergenfurniturenj.com/

For slab doors of that size, solid flatsawn oak will definitely move with the seasons, especially if you’re doing deep V-grooves on one side. To minimize warping, consider a balanced approach: you could make a thin stave or laminated core with solid oak faces, so the grooves aren’t cutting all the way through a single board. Another option is to CNC both sides to balance stress, though that doubles the work. Proper acclimation of the wood before cutting is also key.

1/22/26       #10: Bevel Slat Door Tips ...
Dave Sochar Member

Make your v-joint full thickness, and make it so it looks as if it is solid wood. Because it is. I would up the thickness to 1-1/8" or so. Across the board, as they say.
Plow into each end of each board about 3/8" to 1/2" x 1-3/4" deep.
This plow will then snugly receive what we call a stile if turned 90 degrees. Glued in place, it will stop the movement of the v-joint and hold outside dimensions stable so you can get proper clearances. Just do not try to clamp the width up tight - leave a bit of room (0.0150") so each board can move within its own orbit - just like hardwood floors.

4/24/26       #11: Bevel Slat Door Tips ...
David William  Member

Website: http://www.bergenfurniturenj.com/

You’re right to be cautious, cutting V-grooves on one face will absolutely introduce imbalance. I’d avoid solid flatsawn for this and go with a balanced panel: either rift/quartersawn stock or a shop-made ply/stave core with similar thickness lamination on both faces. Even a shallow relief pass on the back can help equalize tension. Keep moisture content stable and finish both sides equally. At that size, a well-built engineered panel will outperform solid every time.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!