Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

PPB fungus

11/16/20       
Elia Bizzarri

Website: http://handtoolwoodworking.com

A couple days ago, someone mentioned that powder post beetles (I'm using the term loosely) bring a fungus (or was it a bacteria?) with them that weakens the wood surrounding the hole. Is that true? If so, how far beyond the hole is weakened? It probably depends...?...

11/17/20       #2: PPB fungus ...
Tom Gardiner

Many beetles and other insects that bore into wood have a symbiotic relationship with fungi. The insect provides the fungi with the food source while the fungi converts the wood to a digestible form for the insect.
Often the fungal contamination is evident in the in the changed appearance of the wood. Spalting is the marbling effect and does weaken the wood. Often there are multiple fungi competing for real estate and you can see the borders of one another with different coloration and fibre damage.

11/18/20       #3: PPB fungus ...
Elia Bizzarri

Interesting! Thanks, Elia

11/19/20       #4: PPB fungus ...
Gene Wengert

Indeed, the ambrosia beetle, which is a PPB that prefers wetter wood, brings the ambrosia fungus with it when it lays the eggs and the fungus is a food source for the larvae when they first hatch. When the beetles exit the wood several weeks later, they drill a hole to the surface and the fungus then is deposited on this exit hole sometimes and makes the hole a darker color on the border or edges. The fungus does not weaken the wood, but certainly a bunch of small exit holes and the tunnels in the wood when the pupa and larva are active would weaken the wood. Other fungi certainly can weaken wood as they eat a wood component...white rot which causes spalting, and brown root fungi are two groups of wood destroying fungi. And some fungi, like blue stain have no important effect on wood strength as they eat on the sugars and starches in the wood and not the wood itself.

11/19/20       #5: PPB fungus ...
Elia Bizzarri

Fascinating!

To be more specific to my situation, I am building Windsor chairs with oak heartwood spindles that sometimes have powder post beetle holes. Is the strength loss just what the beetle removes, or should I be worried about fungal decay around the hole (besides any decay that I can see with the naked eye; i.e. spalting sapwood, etc.)


View higher quality, full size image (500 X 625)

11/19/20       #6: PPB fungus ...
rich c

The issue with true powder post beetles is not the tiny hole. It's the long channels in the wood under the surface. I've seen infested wood that you could break up with your hands. I would definitely not use that in thin spindle work. In fact most windsor chair makers rive the spindles out of the log so the grain runs the entire length and has the springy characteristic needed for the most comfortable chairs. And red oak can also be brash and brittle compared to woods like hickory.

11/19/20       #7: PPB fungus ...
Gene Wengert

I agree with rich c.

Brash oak will be found in slow growth wood (more than 7 rings per inch). Also brashness results when oak has been dried at too high a temperature (over 160 F) or down to a MC under 7.0% MC.

Even a few degrees of grain angle substantially weakens the wood. So, it is indeed critical that the dowels or spindles always be sawn parallel to the grain, the grain direction is determined by splitting a log and then sawing parallel to the split surfaces.

11/20/20       #8: PPB fungus ...
Elia Bizzarri

I understand all that. I rive my stock, shave it with a drawknife following the grain perfectly, use fast grown oak, dry it at 140F.

If I have a single powder-post beetle hole in the 5/16 diameter tip of a white oak spindle, do you think I should consider the strength loss to be the size of the hole, or is there a possibility that the wood surrounding the hole is weakened.

There are no major unseen tunnels beneath the spindle's surface, since the beetle activity ended when I made the spindle (I put the spindle in the kiln right after making them).

Thanks!
Elia

11/20/20       #9: PPB fungus ...
rich c

The hole you see is the exit hole. An egg is laid, the larva forms and works it's way into the wood to feed and grow. When it's mature it bores out of the wood and repeats the life cycle of mating and the females lays more eggs. If it's powder post beetle, there are ALWAYS channels under the hole, unless you were lucky enough to cut off all the tunnels and you only have the exit hole left. If you don't see channels anywhere, it's probably not PPB. The spindles could easily be tested if the hole causes issues with breaking a couple to test strength. Better to find out before shipping to a customer. As a caution, the center of the wood must reach a minimum of 133 degrees. Most kiln operators sterilize at 150 degrees to insure complete sterilization of the interior of the wood.

11/20/20       #10: PPB fungus ...
Gene Wengert

Have you ever looked at the floor joists from the basement. You see large holes where the wires go through, but these holes are halfway between the top and bottom of the joist. Put the same size hole near the bottom and you have serious strength loss. So, the multitude of tunnels can easily cause strength loss because of their location and the number of tunnels.. The fungus is not "eating the wood" so that is not an issue.

The ambrosia PPB can be avoided in drying by using good sanitation practices (no wood debris) and using recently sterilized stickers, 4x4, etc. in other words, we disrupt their life cycle and also the supply of new insects.

11/25/20       #11: PPB fungus ...
Elia Bizzarri

Thank you!

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery

    Become a Sponsor today!