Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Spindle shaper bearings

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Spindle shaper bearings

10/22/14       
MarcP

What type of bearings are used in high quality production machines?

I have a POS Powermatic PM 2700 5hp shaper that I bought new about 5-6 years ago and I need to replace the bearings for the second time. The first time I had a bearing seize, and Powermatic sent me a whole spindle assembly under warranty.

It seems like the lower bearing is in worse shape than the top bearing, probably because of the side loading the belt puts on the bearing.

I'm thinking about ordering a quill and shaft from Powermatic, and having a machine shop install high quality bearings on the shaft. The stock bearings from Powermatic are ball bearings, obviously of low quality. I'm thinking of asking the machine shop if they could use a high quality roller bearing on the bottom, and a roller thrust bearing on the top side. It seems like with the ball bearing, there just isn't enough support to make the assembly last.

What type of bearings do real shapers use?

10/22/14       #2: Spindle shaper bearings ...
JeffD

It's not so much the type of bearings as it is the size. Your machine probably uses the same bearings the old 26/27's did? Fine for a lot of work, but not to be compared with the "high quality production machines".

For some perspective, this is the bearing from a larger Martin/SCM shaper….with the little guy sitting inside being the bearing from a Powermatic 27. The other pic is of the quill from a Powermatic next to a Martin. This is a large part of what makes a high quality production machine what it is.

Point being that there's no bearing that will make your light duty machine into a production machine. In my opinion your best bet is to replace the bearings and use the machine until you can find yourself a larger replacement. Oh and FWIW the bearings Powermatic used back then were of pretty good quality, not sure if they went cheaper on the newer 2700's though?

good luck,
JeffD


View higher quality, full size image (640 X 478)


View higher quality, full size image (640 X 480)

10/22/14       #3: Spindle shaper bearings ...
MarcP

Great pictures Jeff! That really puts things into perspective!

10/23/14       #4: Spindle shaper bearings ...
David R Sochar Member

If you contact the people at Bearings Inc, they can get you a grade or three better than what you are replacing, as well as advise you on the better choices. They have outlets in most larger cities. They are very knowledgeable folks, but you better move fast as they are closing outlets all over the US with the internet underpricing them all. You may pay a couple of bucks more per unit, but you get solid knowledge and advise along with the part.

Jeff's point is clear - it ain't only bearings. I had a Powermatic shaper that had the quill's vertical movement in dovetailed ways. While the ways were adjustable, the whole thing had all the weight on one side, so the ways wore extremely fast, and they were almost impossible to lube. As a result, it was common for the guy that got stuck using it (instead of the preferred SCMI) to grab the spindle to see if it wobbled before he turned it on. If it was loose, then he'd go underneath and try to tighten the ways. The worst design ever for a shaper.

JeffD - You have a future in machine sales. Good machines, that is.

Bearings Inc.

12/14/14       #5: Spindle shaper bearings ...
MarcP

Well, got my machine apart yesterday and I wasn't too happy with what I found. Seems as though the shaft is undersized, or the bearings are oversized. It appears that the bearings are spinning on the shaft. Not happy. Looks like this machine will need a new quill assembly once a year.


View higher quality, full size image (3264 X 2448)


View higher quality, full size image (3264 X 2448)


View higher quality, full size image (3264 X 2448)

12/16/14       #6: Spindle shaper bearings ...
Larry

Jeff is right on. The PM is a low priced Chinese machine. Generally you can find good SCM, SAC, Gomad, etc. shapers, used for little more than new PM. I've got all 3 of those brands and they are night and day different than the PM. (had a PM26) Time is $. Don't waste anymore on the PM, lesson learned?

12/16/14       #7: Spindle shaper bearings ...
MarcP

Lesson learned, but unfortunately I'm stuck with what I've got. I picked up an OEM complete quill/spindle assembly on Monday, and dropped off the damaged assembly with the machinist. He's going to repair the damaged shaft, press on a stock sized ball bearing on the top. On the bottom of the shaft, a larger roller bearing will be installed. The bottom side of the quill will need to be machined to accommodate the larger bearing. The bottom will be getting a 40mm x 80 mm x 19mm roller bearing as opposed to the factory 40mm x 68mm x 15mm ball bearing. I'll post some pictures when I get it back.

12/16/14       #8: Spindle shaper bearings ...
Larry

I'm not sure the roller bearing is a good idea. Every quill assembly I've had apart uses ball bearings. The bearings are arranged so they can provide pre-load and keep the shaft from moving axially. Star washers, that provide an axial pre-load, allow the shaft to expand and contract when temperature changes occur. Tapered roller bearings could provide preload, but I've never seen them used on a woodworking spindle.

12/16/14       #9: Spindle shaper bearings ...
MarcP

You might be right Larry.

I'm not sure how much the lower bearing contributes to axial support with in the PM 2700 quill though. If you look at the picture I posted with the indicator in it, you can see the exposed lower bearing. Directly above the bearing is a wave washer, which I assume is to preload the upper bearing for axial loads.

Does that sound right?

12/16/14       #10: Spindle shaper bearings ...
Larry

Sounds right, but that seems like a very low pre-load. Some of the assemblies I've had apart use angular contact ball bearings so they can stand a high pre-load.

12/16/14       #11: Spindle shaper bearings ...
MarcP

Let me quote your first post.

Jeff is right on. The PM is a low priced Chinese machine.

:-)

12/17/14       #12: Spindle shaper bearings ...
JeffD

Sounds like you may be too far along already, but I would re-think having a bunch of expensive machine work done on that one, and instead put that money aside towards a bigger machine. As long as you have the new quill assembly you should be able to get some decent life out of it, giving you some time to shop around for something a little beefier. Better than throwing good money after bad on a light duty machine anyway.

There's a lot of big shapers sitting out there with apparently very few buyers. Don't know where your located but there's a Delta R-15 shaper (that I think comes with the feeder too) near me the guy can't give away for $2k! Total buyers market these days….for shapers anyway.

good luck,
JeffD

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)