peel and stick veneer, does it hold up?

1/29/13       
dan

Does it stay attached or will it let loose after time. Looking at a quick way for finished ends on cabinets. Currently I apply 1/4 inch ply with contact cement and am curious if this veneer would do the job or if it's not a good product.

1/30/13       #2: peel and stick veneer, does it hold ...
Charles  Member

Website: http://www.northcreekwoodworks.com

Never used it (never will). Sounds sketchy. I doubt it will last forever.

1/30/13       #3: peel and stick veneer, does it hold ...
Kamil Antos Member

Website: http://www.wisewoodveneer.com/

Dan,

There are a lot of mixed feelings about the "peel and stick" veneer. I know there are a lot of traditionalists that won't even look at paperbacked veneer, let alone the peel and stick or PSA veneer. I am aware of the myriad ways to apply different veneer and veneer products. Some methods are better suited than others for different situations. Ultimately the choice is yours whether a product will work for you or not. The PSA backed veneer is convenient when you have to work in the field and on cabinets that are already installed.

Here are some facts about PSA veneer:

PSA stands for pressure sensitive adhesive, it is a viable product and has been used by many (including myself) with success. Its bonding strength comes from the application of pressure. With this type of adhesive this can only be done by hand. Very similar to how you would use contact cement. The application of this pressure is paramount for the successful application and use of PSA veneer. You should not use a J roller with this product. A veneer scraper or veneer hammer is the tool of choice. The pressure should be as firm as possible and scraped with the direction of the grain. Repeating the application of pressure is crucial. You cannot apply too much pressure and with certain veneer species it would be wise to repeat the process several times (maple is notorious). The PSA requires a lot of psi, this will help to restrain the veneer from moving with the changes in humidity. The 3M PSA also works better on less porous surfaces. As with all veneer application methods, surface preparation is important.
The relative ease of use with this type of veneer and adhesive is misleading. Some users grossly underestimate the application process. Veneer with this adhesive is not a sticker or shelf paper. The name “peel and stick” oversimplifies the process and lowers the user’s expectations. There is no shortcut as to how meticulous the application process is. If you are doing it right than you will be breaking a sweat. Applying PSA veneer can become very labor intensive especially on large projects and in those circumstances you might find that other and more traditional application methods are better.

I have cabinets I built over 10 years ago and used cherry 3M PSA veneer over a plywood substrate. I have yet to have an issue with the veneer. We sell to door manufacturers that use PSA veneer on steel doors for commercial applications. They have extensively and rigorously tested the pressure sensitive adhesive under circumstances exceeding everyday use.

My comments are not meant to start a qualitative argument with the professionals that stick only to traditional methods, as far as which method of veneering is better. They are meant to be informative so you can make a better decision.

Good luck.

2/1/13       #4: peel and stick veneer, does it hold ...
Kilgore Trout Member

If you look at your work in the context of time, it may help you decide. There is also a historical context.

If your work is expected to last lifetimes, then more robust standards apply that would certainly exclude peel and stick or contact. If your work is short-lived - destined to be removed in a few years, or end up on the curb, then perhaps peel and stick/contact is a viable method. Of course, this assumes you are okay with disposable resources - your time and the wood products.

Historically, veneer slicers outpaced glues in the early 20th century and made for a lot of furniture that was 'papered' over with veneer to dress it up. The poor quality glues caused the veneers to catch and peel, and gave veneer a bad name. It wasn't until after WW2 that glues became better and techniques advanced to make a better veneered product. However, the notion of 'cheap veneer' is still out there.

I think you will find that better craftsmen (better in the eyes of their peers) and professionals will use presses and more industrial methods of veneer application, and those that are new, naive or unaware are more likely to use peel and stick or contact cement.

2/1/13       #5: peel and stick veneer, does it hold ...
ThomasFR

Kilgore, not bad counsel but your "historical context" demands correction. Hide glue, used nearly exclusively for hundreds of years is not & has never been inferior & is not to be blamed for veneer failure of shoddy 20th century "short-cut mass production" goods. It is obvious to the most casual observer of "great" antique veneered furniture made in the 17th & 18th century, currently in daily use in probably thousands of homes & certainly in museums worldwide that hide glue is & has been more than adequate for "lifetimes" of use!

2/1/13       #6: peel and stick veneer, does it hold ...
Kilgore Trout Member

Thomas FR - I stand corrected. Actually, I'm sitting, but ....

You are correct - Hide glue is a very good and more than adequate glue when used properly and with the intention of making a quality product. Yes, an army of deceased cabinetmakers and eboniste` would be on me for eternity for such casual dismissal of their methods.

I should have said that the methods used to 'wrap' a piece with veneer caused problems with corners lifting and catching. This was also during the post industrial revolution and the birth of consumer products that demanded lower cost methods of production. The shorter life expectancy and resulting perception of cheap were side effects of the larger forces at work.

One might see a correlation with the peel and stick of today and the current demand for ever cheaper goods.

Thanks for the correction.

2/19/13       #7: peel and stick veneer, does it hold ...
Chaim Gottesman

Kamil, can you explain why a J roller is not a good idea to apply the PSA veneer?
I would think that a veneer hammer could leave indents in the veneer.
is there a "primmer" that can be used for the surface of the substrate?
Thanks,
Chaim

2/19/13       #8: peel and stick veneer, does it hold ...
Kamil Antos Member

Website: http://www.wisewoodveneer.com/

Chaim,

A J roller will not give you enough pressure on the glue line to ensure the veneer is as stable as possible. A tapered and pointed blade, slightly eased to 1/16" radius, will give you much more pounds per square inch. A veneer hammer is such a tool. You can also make a veneer scraper out of 1 x 3 stock by cutting one end of 16" length on a 45 degree angle and easing the point. Always scrape with the grain. The reason it is crucial to administer as much pressure as possible is that PSA is a PRESSURE SENSITIVE adhesive. The more pressure the more stable the glue line will be. A stable glue line will help keep the veneer from moving and changing with environmental conditions.

As far as a primer for your substrate: if the substrate is porous you can seal it with a coat of lacquer or sanding sealer. Make sure the substrate is as smooth as possible. Any flaw in the surface can potentially telegraph through the face of the veneer.

4/17/13       #9: peel and stick veneer, does it hold ...
Jim Member

Website: http://www.new-look-kitchen.com

Been using PSA veneer for over 20 years with-out any serious problems occurring. Many die hards are against it's use but I am happy with it. I am in the Chicago area and have refaced over 2000 kitchens personally so far in my career. Other than some that's out of my control like the original cabinet foundations shifting I am very satisfied..
NOBODY EVER WANTS CALL BACK COMPLAINTS for a repair...


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)