In this issue:
WOODWEB Anniversary Poll
2015 represents the 20th year that WOODWEB has been in service, and we're interested in finding out how long woodworkers have been visiting the site. Let us know by voting in our latest poll - current results for the poll will be displayed immediately after voting, and you may return and view results at any time by clicking the "Vote Now and View Results" link.
http://www.woodweb.com/cgi-bin/forums/cabinetmaking.pl?read=771911
Hot Threads
A walnut end grain counter top is cupping despite the use of multiple glue methods. Check out the advice shared to solve the cupping problem.
http://www.woodweb.com/cgi-bin/forums/aw.pl?read=771584
Inefficiency is bogging down this shop's productivity. Follow
the suggestions from fellow shop owners to help streamline
operation.
http://www.woodweb.com/cgi-bin/forums/business.pl?read=771424
Double stacking cutters on a shaper is the question at hand. See if setting up positive stops will enable back and forth work with both profiles.
http://www.woodweb.com/cgi-bin/forums/cabinetmaking.pl?read=771492

A 3 phase CNC is being introduced to a single phase shop. Should the shop owner upgrade service or install a converter?
http://www.woodweb.com/cgi-bin/forums/swmf.pl?read=771461
Featured Project
This Acoustic Guitar was recently posted at the Project Gallery:
http://www.woodweb.com/galleries/project/posts/4497.html

Recent Additions to
the Woodworkers Directory
The following companies recently created
free web pages at the
Woodworkers Directory. Create yours at:
http://www.woodindustry.com/woodworkers/index.html
Pomeroy Lumber Products, Inc.
http://www.woodindustry.com/woodworkers/Master/10620.html
All Flooring and Window Treatments
http://www.woodindustry.com/woodworkers/Master/10622.html
JMF Construction, LLC
http://www.woodindustry.com/woodworkers/Master/10623.html
Web Marketing 101 FAQ's are a great way to make your
customers more comfortable with you or your business. Make sure you are answering real "frequently asked questions", and not just the ones you wish customers
would ask. It's not about marketing fluff, but answering real concerns that can win you business. FAQs Still Deliver Great Value
|
This issue of the WOODWEB Update is
sponsored in part by KCD Software:
KCD Software is an award-winning manufacturer of custom software
designed to facilitate woodworkers, designers, builders and renovators
of cabinetry and closets. Visit our website at:
http://www.kcdsoftware.com/CCD-try.html
|
Knowledge Base Highlights
See a complete list of the most recent additions
to our Knowledge Base at:
http://woodweb.com/Resources/RSMostRecentKBArticles.html
As plywood quality declines, finishing problems multiply. Here's a look at why plywood is so hard to finish these days.
http://www.woodweb.com/knowledge_base/Appearance_Defects_with_Waterborne_Finishes.html
A cabinetmaker receives feedback on the idea of targeting smaller and less expensive jobs.
http://www.woodweb.com/knowledge_base/Shifting_to_a_LowerPriced_Cabinet_Market_Segment.html

Here is some background information and an extensive set of photo examples of finished solid sheet acrylic and acrylic veneer work.
http://www.woodweb.com/knowledge_base/Making_Acrylic_Cabinetry.html

Finishers share views on the selection and
application of solid-color finishes for kitchen cabinetry.
http://www.woodweb.com/knowledge_base/Solid_Color_Finishes_for_Kitchens.html
Relocating to a larger shop space involves complicated pros and cons, including commute times, neighbor relations, marketing implications and more.
http://www.woodweb.com/knowledge_base/Whether_to_Move_the_Shop.html
Video Pick
Veneer Systems Inc. features a Hofer Koptronik
case
clamp demo. To view the video, click on the link below
and scroll down to the Veneer Systems Inc. video link:
http://www.woodweb.com/VideoLibrary/VLAlpha.html
To UN-subscribe, change your address, or
contact WOODWEB, follow the
instructions at the end of this message. Replies to this Update mailing
will
not reach WOODWEB.
Find out how to promote your company on
the Web. If you're a supplier to
the wood industry, visit WOODWEB's Media Kit:
http://www.woodweb.com/MediaKit/MKindex.html
If you're a woodworking professional, visit
the Woodworker's Directory:
http://www.woodindustry.com
View past WOODWEB Updates at:
http://www.woodweb.com/update_archive
The WOODWEB Update is Copyright (c) WOODWEB,
Inc. 2015
http://www.woodweb.com
|