Lumber Weight Calculator



Recalculate the weight of your lumber
at a revised Moisture Content (MC)

The original MC you entered was: 20%
The original Board Footage was: 19565 Bd Ft
The resulting weight was: 42652 lbs

Recalculate weight at a new MC of: %




View "Weights of Wood" Chart

Instructions: Lumber Weight Calculator

Moisture Content:
Enter the moisture content (MC) at which the lumber was scaled (i.e. when the board foot volume was measured). Decimal values are acceptable. Do not enter fractions, and do not enter the percentage sign after the value.

No. of Board Feet:
Enter the board footage value as measured at the moisture content (MC) indicated in the Moister Content field above. Leaving the board footage value at the default (1000) will produce a resulting weight in pounds per 1000 board feet. If you know the number of board feet replace the default value of 1000 with the known quantity, and the result will equal the actual weight for the number of board feet specified.

Actual Width:
Enter the actual measured width of the lumber, in inches and fractions of an inch.

Nominal Width:
Enter the nominal measured width of the lumber, in inches (and fractions of an inch if appropriate).

Actual Thickness:
Enter the actual measured thickness of the lumber, in inches and fractions of an inch.

Nominal Thickness:
Chose a nominal thickness of lumber. Lumber less than 3/4 inches thick should be entered as 3/4.

Actual Length:
Enter the length to the last full foot. Do not round up to the next foot. Any inches entered will not be considered in the calculation.

"Calculating the weight of lumber" is a detailed article regarding the calculation of Lumber Weight. If you have any questions regarding the methodology used in WOODWEB's Lumber Weight calculator, we suggest that you post your question at our
Sawing and Drying Forum.

You may also want to review our "Weights of Woods" chart ... if you know the total board footage value you can use this chart to determine the estimated weight.

Click Here to Access the Lumber Weight Calculator




Today's Sponsors
  • Colonial Saw
    North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
  • Forestry.com
    Forestry.com is a specialized platform with educational content and equipment for Loggers and Foresters
  • Safety Speed Manufacturing
    Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
  • American Vision Cabinets
    Leading provider of Custom CNC cabinet parts and components and Edge banding services
  • Elias Woodwork & Manufacturing
    Solid Wood Cabinet Doors, Furniture, Dovetail Drawers, Mouldings, and Related Items
  • TotalFinishingSUPPLIES.com
    Solutions and supplies from spray tips to spray booths for all your woodworking needs
  • WOODWEB, Inc.
    The Information Resource for the Woodworking Industries
  • VortexTool Co. Inc.
    Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
  • O'Shea Lumber Company
    Merchants of Fine Woods
  • TradeJobPlacement.com
    Individualized Placement Services, Specializing in Millwork Design Engineers
  • Simantech
    New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
  • Scarlett Machinery Inc.
    New and Used CNC Routers and Used Woodworking Machinery, for Operations Ranging From Small Woodworking Shops to Large Progressive Manufacturing Plants
  • Shop Gear Inc.
    Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America

Become a Sponsor today!