Just finished building the inlay and installing this french knot in a dining room floor. The pin striping is maple, the edges are walnut and the center is quarter saw sycamore.I laminated these 1/4" strips to plywood then t&g them in the shaper.

2 Photos
Social Media:
Viewer Comments:
Posted By:Harry DeVrieze
Very nice. Makes you want to step up to get out of the room.