Viewer Comments: Posted By:
John[01/28/2007]
I like the clean and simple look. What type of method did you use to construct the boxes? I assume the drawer boxes are melamine. Did you use pocket holes to assemble them? Did you apply the edgebandig by hand or did you use an edgebander? Nice job.
Thanks,
John
Posted By:
Michele[01/28/2007]
I use a melamine glue then tack with brads then screw all boxes. Unfortunately I have to do all edging by hand but one day will have an edgebander. I use end panels on all exposed ends to cover screws. Thanks for the comments, always appreciated.