      What's a suitable adhesive for attaching a new plywood end panel to an existing cabinet? September 22, 2005

I am in the process of building new base cabinets for a kitchen where the owners are keeping their old wall cabinets. I was unable to find any 3/4" material that had the same grain, but I did find it in a 1/4" plywood, so I decided that in order to match the wood grain of the old cabinets,
I have to skin the outside finished ends with 1/4" plywood (birch).

My question is this - what is the best method to glue the 1/4" plywood to the 3/4" unfinished plywood? I tried using yellow glue, but its very difficult to get good contact uniformly. I know I could use contact cement to get better uniform contact, but is it a good long term solution?

Forum Responses
(Cabinetmaking Forum)
From contributor J:
It works on plywood laminate - and what else would you do? This is how re-facing goes. I don’t know the clients, but the way the housing trends go you should ask yourself if a perspective home buyer in ten or fifteen years even be using the existing kitchen.? I am suggesting that you look at the possibility that the longevity of something like this is fairly subjective.

From contributor V:
I don’t think there is anything wrong with contact cementing a .25" skin-on.

From contributor F:
I use PVA and FSV, a fast tack PVA emulsion for most ends, 2 ply veneer, 1/4" ply and 1/4" one sided melamine. These allow moving the applied end for good location and fit and in the end I have a non creeping hard glue line. Clamping can be tricky once in a while, but a couple of well place blocks seem to solve all of these problems. The clamps can be removed in twenty minutes with FSV and about an hour with PVA, some time sooner in my hot dry climate.

From contributor M:
I don't think I would use contact cement. There is a big difference in the expansion rates for the two items. I've been told that under no circumstances should contact cement be used to apply veneers, so I would think that rule would apply in this case.

From contributor V:
Veneering is when you adhere very thin (.0625" or less basically) solid wood pieces to a substrate. Contact cement is not used in better work of this nature. When you are using veneered plywood, the veneering is already done. I think a lot of people confuse laminating with veneering. From what I read in the original post, the questioner wants to attach plywood to plywood (similar expansion). I would not hesitate to use contact cement to adhere .25" plywood to other plywood, MDF, or particle board.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: General

  • KnowledgeBase: Cabinetmaking: Installation

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2017 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article