Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Bonding Stainless Steel to Plywood       Advice on fabricating a stainless-steel-on-plywood tabletop. June 28, 2007

Question
I'm building a conference table for an architect: a stainless steel top glued flush to a double 3/4" layer of appleply, the ply edges showing for a high tech look. Contact cement means the steel has to go down perfectly - any other ideas? If I cut the ply a little large, I can sand the edges back to the steel. Any better suggestions?

Forum Responses
(Adhesive Forum)
From contributor T:
I would try a smaller piece of steel on wood to make sure it will hold properly. If it does, cutting the plywood large to begin with is a good idea. Then trim it close with a saw. Then use a trim router bit to do the final finish. If you don't have one the full length of the ply, then use a pattern router bit on the steel side, then turn the tabletop over and use a flush trim in the previous cut. You could also use a router bushing to trim away from the steel and 45 the edge with a bearing piloted bit in the trim cut. The cuts would have to be real close, but may give even a better appearance.



From contributor B:
Whatever you use for glue, consider balancing this sandwich with a sheet of cheaper sheet metal on the underside. That should make one nice flat plate.


From contributor A:
I have used pl premium on many different things including glass to stainless steel, frozen lumber and many others. Try a test piece out yourself - has great holding power. I would suggest using a fine notched trowel and not too much glue towards the final edge. Glue has a fair open time and cleans off easily when wet with thinners. I have used it on a steel top bench for a bearing distributor - been on 5 years and ain't gonna let go any time soon!


From contributor B:
You might look into using a thin layer of thinset adhesive used for attaching metallic tiles. This should allow some tweaking of the final position.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Adhesives, Gluing and Laminating

  • KnowledgeBase: Adhesives, Gluing and Laminating: Glues and Bonding Agents

  • KnowledgeBase: Furniture

  • KnowledgeBase: Furniture: Custom Furniture




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article