Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Claro Walnut Characteristics       Details on the origin and behavior of Claro Walnut wood. October 23, 2007

Question
I am bidding on turning a few hundred stair balusters in walnut. I put out a RFQ with Wood Planet for the blanks and got a call from a supplier of Claro walnut. Do you know anything about this walnut? Ever used it? Is it a true walnut?

Forum Responses
(Architectural Woodworking Forum)
From contributor T:
Yes, it's a true walnut, usually English walnut that was grafted on another walnut root stock (black walnut or California walnut). It is nice looking, usually shorter lengths as it typically comes from old orchard trees. Most of it is not steamed, so sapwood could be an issue and the color is not right to use as a substitute for black walnut unless the customer agreed up front.



From Professor Gene Wengert, Sawing and Drying Forum technical advisor:
Claro walnut is called Juglans californica. It is native to the USA. Common names include California black walnut, California walnut, claro walnut, southern California walnut. I do believe that this is the species you were offered. Claro walnut lumber would most often come from walnut orchard trees, so grain and color can be variable indeed. Note that it is a species all by itself, grown in Western U.S., and produces claro walnut lumber.

Sometimes, claro walnut is grafted to the root stock of English walnut. This might be the source of information on the previous posting. This would be rare in the U.S. Sometimes claro root stock has English walnut grafted to it because the roots are resistant to decay and the top produces tasty sweet walnuts.



From contributor F:
Being out west and having worked extensively with Claro walnut, I can tell you that English walnut is often grafted on to claro root stock and I have never seen the opposite. The reason for the grafting is that the claro root is heartier in this climate and soil and the English nuts are preferred because the shell is thinner and the yield of nut meat is much higher than from the black/claro which have thick shells and smaller nut meats. Although the trees the stock comes from are most often orchard trees, the trees grow rather large and the lumber is available in very long lengths and many thicknesses. Other than that, I can only say that this wood is beautiful and often figured when from a large tree. A real pleasure to work with. The English is different entirely and very pale in comparison.


The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor S:
Claro walnut is a misused term; it has been misused for so long there is no turning back. Originally, it referred to the root stock below the graft line on English walnut trees in orchards as contributor F said (above). The root is where you get heavy compression figure and color that is prized for gun stocks.

Today, however, many refer to all western walnut as Claro to differentiate from its eastern cousin Juglans Nigra (which is a commodity hardwood and the western species is not, which means a big money difference). It is my understanding that the root stock used in orchards is a native walnut species Juglans Hansii. English walnut has a tendency to rot so using the native species adds life of the tree.

In Oregon, it is not uncommon to find Juglans Hansii in whole tree form. It is apparent by its small, round, quarter sized, thick shelled nut (also stated above). They typically do grow to be large trees but I suspect that some of the difference between it and the eastern species has a lot to do with environment. I say that because there are occasions when we have harvested an eastern walnut tree and the lumber turns out with less color variation but still beautiful colorful wood. The Claro color has to do with the species but in my opinion it also has much to do with how it is dried. The entire process of harvesting and drying is different making western walnut lumber a unique and independent product from eastern walnut. We air dry our lumber one season (summer to summer) per inch. After that we can use our dehumidifying kiln to extract moisture getting the wood down to 6-8%. It is most common to find eastern walnut dried in a steam kiln. Steaming bleeds the tannins from the heartwood into the sapwood, which allows a higher grade of lumber.

Many believe that Claro is a California species but we have seen many Juglans Hansii as far north as British Columbia. Harvesting Claro logs allows us to cut lumber in standard lengths (6’, 8’, 10’ and sometimes 12’). It is not usual for the butt cut to yield a log over 20 feet long.

In the Pacific NW walnut trees often stand alone either in a field, yard, along roads or in a parking lot. Point is they have room to grow and in very good soil and climate conditions. In the east, however, while you do get the occasional stand alone tree, most are harvested from a forest. In a forest, trees grow up rather than out.



Comment from contributor A:
We have been harvesting and selling western walnut for 33 years here in Oregon. I think the correct description of our walnut is that it is a hybrid of Juglans Nigra and Juglans Hindsii. It is similar in color and figure to the "California Claro" but is denser with the strength characteristics of American black walnut. Most of the trees we see are not orchard graft stock and are from 24" to 72" in diameter with useful logs up to 25' long.

A typical mill log would be 36" in diameter and 12' long. We air dry 1" per year and use a DH kiln to complete the process and take lumber down to 6% - 8% moisture content. Western walnut typically sells for a 30% to 50% premium over American black walnut.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Wood Identification

  • KnowledgeBase: Wood Engineering

  • KnowledgeBase: Wood Engineering: Wood Properties




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article