Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Converting log volume scales       When sellers and buyers want numbers in different scales, how do you come up with the calculations? July 22, 2003

Question
I have a problem on my hands. I have a seller that wants me to take logs in Doyle Scale. I have buyers that want everything laid out for them in International Scale or Scribner Scale. Can someone help with the conversion of Doyle Scale to both International and Scribner scales?

Answer
(Sawing and Drying Forum)
Buy on the Doyle rule, and sell on the Int'l 1/4". Your logs will yield more bd. ft. in the process.



From the original questioner:
I don't know what you mean by "sell on the Int'l 1/4"... is that another scale?


International scale is really called the International 1/4-inch scale. There is also the Int-1/8" scale.

As all the scales are represented by formulae, it is easy to convert one to the other.

I have never seen Scribner used except in the West and they do not use Doyle there. Please tell me where you find people using all three scales? In fact, using Int 1/4 is also not common. I will send you a conversion table, but it is dependent on diameter, so there is not a one number conversion.

Gene Wengert, forum technical advisor



I found that the WOODWEB calculators work well for me. It takes awhile to put in all your logs and such, but you will get used to it. I too struggle with all the different ways that people use to measure logs and timber. Here we use good old cubic meters (424bft per m3).


Contact Wood-Mizer - they have a pocket slide ruler that has all three on it.


From the original questioner:
Sorry to confuse you. Here's the situation. I have a seller who is trying to sell logs to me by the Doyle scale. I have buyers overseas that are using what they call the "American MBF scale," which I assumed is the Scribner or International Scale.

The logs that I am interested in are 16", 17", 18" and 19" x 8', 9' and 10'.



I would make sure what scale they are talking about. We do a lot of export, and it's all Doyle scale. The price is relative to scale.


The Doyle scale is calculated as follows: (diameter-4)^2= board feet in a 16 foot log. To find the scale on other lengths, just divide that number by 16 and multiply the length.


If you look in the Knowledge Base here at WOODWEB (enter a keyword such as "scales" in the search box at the top of the page), you will find several good past articles.

Included in one article are volume tables for International and Scribner:
http://www.woodweb.com/knowledge_base/Log_Volume.html

Another includes the formula for all three log rules (given below). Formula (Doyle, Scribner, and International) for log volume:
http://www.woodweb.com/knowledge_base/Estimating_BF_yields.html

Gene Wengert, forum technical advisor



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Business

  • KnowledgeBase: Business: Estimating/Accounting/Profitability

  • KnowledgeBase: Business: Sales

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Buying

  • KnowledgeBase: Primary Processing: General

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Yield Formulas




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article