Today's
Sponsors:


Vintage Wood Products

VortexTool Co. Inc.

VyTek

W. Moore Profiles, Ltd.

W.L. Fuller

Wagner Electronic Products

WalzCraft Industries

WEIMA America, Inc.

Weinig Group - USA

Western Dovetail

Williams and Hussey

Wisconsin Knife Works

WMIA

WMMA

Wood Doctor's Rx, LLC

Wood Technology Inc

Wood-Mizer

WoodCabinetDoors.Com

WoodenBoat

WoodFinder

WoodJobs.com Search Consultants

WoodLINKS

Woodmaster

WoodPlanet Inc.

WoodSprayGuns.com

WOODWEB

Woodworker's Supply/woodworker.com

Woodworker's Directory

Woodworking in America

Wright Timber

Specialtytools.com

Speed Sander

Spink Lumber

Sprayguncaptain.com

Stefani

Steve H. Wall Lumber Co.

Stiles Machinery

Stiles Shop Solutions

Stoneys Hardwoods

Super Source Tooling Inc.

Supergrit Abrasives

Superior Wood Products

T-Tool USA LLC

Target Coatings

TaylorCraft Cabinet Door Company

Techno CNC Routers

Template Services

The Veneer Store

Thermwood Corporation

Tiger Wood Ltd.

TigerStop

TigerwoodDecking.com

TimberKing

Timesavers Inc.

TMS Machinery Sales

Tomlin Architectural Millwork

Tooling on the Web

Toolstoday.com

Top Drawer

Touch Up Solutions LLC

Tractivity

TradeJobPlacement.com

TradeSoft

Trakware Systems Inc.

TRB Flooring Company

Tropical Hardwoods

True North Cedar

Ubidmachinery Inc.

UC Coatings Corp.

Unique Building Supples

Unique Machine & Tool

University of Wisconsin

UWMO Auctions

VacDry Kilns

Vacuum Pressing Systems, Inc.

Vacuumpods.com

Valspar

Vecoplan LLC

Vector Art 3D

Vectric Ltd.

Veneer Systems Inc.




Cutter Profiles for Tongue-and-Groove Flooring       Tips on the fine points of profiling tongue-and-groove floorboards. September 10, 2007

Question
I'm about to make 1000 sq. ft. of flooring for the first time but I'm very nervous about shrinkage and how it goes together. I'm using red oak kiln dried to 8 percent. But my question is about the type of cutters to use. I'll be cutting it on a WM 718. I have the option to mount two routers at the end and use it as a 3 sided planer, or I could just run it through one operation at a time. I've been looking at a lot of different profiles but I've noticed that some, like the Grizzly c2307 and c3699z, both have a 1/32 taper on one side. This looks great for the install, but what about when it's sanded - won't this start to form a gap the more it gets sanded? These cutters also do not have an undercut for the nail or staple. Is this an issue? If anyone uses a type of cutter or router bit that works well, I would love to know.

Forum Responses
(Solid Wood Machining Forum)
From contributor C:
A true flooring profile has 2 distinct differences from just T+G. First, the edge below the groove (the bottom face, if you will) is typically 1/32 narrower than the top. This is so that the exposed joint, the top, can always come together without interference from the bottom edge. As far as its opening up post sanding, you would have to sand through the T+G 1st to get to the gap, which I think would be more noticeable than a 1/32 gap. And how many times are you planning on sanding this? I offset the T+G about 1/16 to the bottom to get a little extra for the people refinishing the floor 80+ years from now...

The other difference is that above the tongue, there is a small groove milled, a nail slot. Flooring nails are flat, and either L or T shaped. This slot allows the head a little extra room to sink, so that like the offset bottom edge, you don't get interference on the exposed joint.

I would think if want to run this in one pass, which you do, you might want to take a look at some of the knife suppliers here on WOODWEB; their profile books will show an illustration of what I'm talking about. Many of the guys here can help you find either a corrugated back head for your machine that will allow you to run any profile you can grind on your side heads, or perhaps dedicated heads would be the way to go.

As long as the house is climate controlled (heat/AC), and insulated well, 8% should be okay. I typically dry our floors to 5-6%, but that's because most go into new high end homes that are buttoned up tight and dry.



From Professor Gene Wengert, Sawing and Drying Forum technical advisor:
I would prefer a little bit lower MC to avoid shrinkage... 7.0% MC with nothing wetter than 7.7% MC if you will install the floor during the heating season. This MC level is about 35% RH.

I am concerned when you state that it was kiln dried to 8% MC. I wonder if there are a few 9% pieces or even wetter. You should get a moisture meter and check the MC so you know both the average MC and the spread of MC around the average. In a kiln of 50,000 BF of lumber (about 10,000 pieces), the operator usually runs the kiln based on only 12 samples. Wetter pieces can happen.



From contributor T:
I have included a picture of a very standard profile for hardwood flooring. It depicts what contributor C was talking about and some other features that many flooring manufacturers use today. The additional features include a rounded tongue and a tapered groove. These features make for easier assembly.


Click here for higher quality, full size image


Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Architectural Millwork

  • KnowledgeBase: Architectural Millwork: Flooring

  • KnowledgeBase: Solid Wood Machining

  • KnowledgeBase: Solid Wood Machining: Tooling




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article