Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Distressing Techniques to Mimic Driftwood       A woodworker seeks advice for creating the shipwreck look. March 17, 2005

Question
I have been given the challenge of building an oak dining table that looks as though it has been in a shipwreck and water has taken its toll. I build exclusively from barn wood, so I have some weathering already. How can you fake the driftwood look?

Forum Responses
(Finishing Forum)
From contributor M:
Bleach, bleach, bleach. Use the two part, oxalic acid, and clorox. Use them all. Have fun, play around. The more messed up it looks, the better. I did a heavily distressed countertop for someone and used all the bleaches as well as potassium dichromate, wax, shellac, boiled linseed oil, water, Orange Crush, and Pepsi. It looked very authentic.



From the original questioner:
I can see bleach, potassium dichromate, wax, shellac and boiled linseed oil. But Orange Crush and Pepsi?


From contributor S:
One other thing that you see on driftwood is uneven wear between harder wood (growth rings) and softer wood. This gives a ridged appearance to the wood, most easily simulated by light sandblasting.


From the original questioner:
Thanks for the great info. But as I do not have the facilities to use such harsh chemicals, can I get away with pressure washing and sand blasting, then just some bleach to lighten it up? And the Orange Crush and Pepsi trick…


From contributor M:
If you're trying to pull off an authentic distression, you must think outside the box and use methods and products you would not normally associate with woodworking. Driftwood is very grey, so how about putting some grey glaze right on the bare wood? Try to find a way to simulate all the little surface checks that driftwood has, maybe with a v-groove chisel, or skimming some parts against your bandsaw blade.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Furniture

  • KnowledgeBase: Furniture: Custom Furniture

  • KnowledgeBase: Woodworking Miscellaneous

  • KnowledgeBase: Woodworking Miscellaneous: Woodworking




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.