Today's
Sponsors:


Vintage Wood Products

VortexTool Co. Inc.

VyTek

W. Moore Profiles, Ltd.

W.L. Fuller

Wagner Electronic Products

WalzCraft Industries

WEIMA America, Inc.

Weinig Group - USA

Western Dovetail

Williams and Hussey

Wisconsin Knife Works

WMIA

WMMA

Wood Doctor's Rx, LLC

Wood Technology Inc

Wood-Mizer

WoodCabinetDoors.Com

WoodenBoat

WoodFinder

WoodJobs.com Search Consultants

WoodLINKS

Woodmaster

WoodPlanet Inc.

WoodSprayGuns.com

WOODWEB

Woodworker's Supply/woodworker.com

Woodworker's Directory

Woodworking in America

Wright Timber

Specialtytools.com

Speed Sander

Spink Lumber

Sprayguncaptain.com

Stefani

Steve H. Wall Lumber Co.

Stiles Machinery

Stiles Shop Solutions

Stoneys Hardwoods

Super Source Tooling Inc.

Supergrit Abrasives

Superior Wood Products

T-Tool USA LLC

Target Coatings

TaylorCraft Cabinet Door Company

Techno CNC Routers

Template Services

The Veneer Store

Thermwood Corporation

Tiger Wood Ltd.

TigerStop

TigerwoodDecking.com

TimberKing

Timesavers Inc.

TMS Machinery Sales

Tomlin Architectural Millwork

Tooling on the Web

Toolstoday.com

Top Drawer

Touch Up Solutions LLC

Tractivity

TradeJobPlacement.com

TradeSoft

Trakware Systems Inc.

TRB Flooring Company

Tropical Hardwoods

True North Cedar

Ubidmachinery Inc.

UC Coatings Corp.

Unique Building Supples

Unique Machine & Tool

University of Wisconsin

UWMO Auctions

VacDry Kilns

Vacuum Pressing Systems, Inc.

Vacuumpods.com

Valspar

Vecoplan LLC

Vector Art 3D

Vectric Ltd.

Veneer Systems Inc.




Door/drawer gaps in Euro-style cabinets       Americans need to apply the looser European standards to door and drawer gaps to avoid frustration when ordering these parts from other manufacturers. October 18, 2000

by Jon Elvrum

Q.
We manufacture European style cabinets, and work with very close tolerances. Our doors are ordered from manufacturers who specialize in door manufacturing only and are supposed to have all of the specialized automated equipment to make these doors to exact specifications.

We have been having a lot of problems getting our doors made to our measurements. When you are working with 1/8" tolerances between doors and drawer fronts, 1/16" differences between what we order and what we get can make a big difference. Also we have a lot of problems getting hardwood raised panel doors that aren't out of square, which also causes problems.

This is quite frustrating when you are trying to put out a quality product, and causes many scheduling delays from having to reorder defective doors.

Do you have any recommendations as to reputable door manufacturers? About 80% of our doors are vinyl wrapped, the rest hardwood raised panel.

A.
A classic problem with converting European styles to American manufacturers is that there is an unnatural desire to be "perfect." The tolerances of 3mm (1/8") is not the tolerance one sees when in Europe.

The European cabinetmaker often works in a 4-5mm gap, which is considerably more forgiving. The 3mm gap which I have preached myself is a near "ideal."

If you are working on an 800mm tall box with 5 drawers, you are looking at a 157mm drawerfront, zero gap at the bottom of the stack and 3mm between the 5 drawers. This leaves 3mm at the top, beneath the counter. If you want a 4mm gap, you simply reduce the drawer head accordingly.

A more common American box would use a top drawer of 160mm - 32 (net 124mm with 4mm gap or 125 with 3mm gap). The main thing is the 3mm decision has always been arbitrary, and in Europe it is rarely followed.

Jon Elvrum, Director of Distribution and Sales at Ritter Manufacturing in Antioch California, is also a well known author and consultant to the cabinetmaking industry. He has written numerous articles on the 32mm cabinetmaking system and production woodworking in general.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Cabinetmaking: Commercial Cabinetry

  • KnowledgeBase: Cabinetmaking: Custom Cabinet Construction

  • KnowledgeBase: Cabinetmaking: Cabinet Design

  • KnowledgeBase: Cabinetmaking: Cabinet Door Construction

  • KnowledgeBase: Cabinetmaking: General

  • KnowledgeBase: Cabinetmaking: Residential Cabinetry

  • KnowledgeBase: Woodworking Miscellaneous: Woodworking

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article